Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 2 | 90.6 - 96.1 °C | 195 - 205 °F | |
Huntsman IROGRAN® A 85 H 4827 TPU-Polyester Introduction: IROGRAN A 85 H 4827 is a thermoplastic polyester polyurethane for injection molding applications. IROGRAN A 85 H 4827 is part of the HUNTSMAN technical injection molding product range .. |