Zone 2 90.6 - 96.1 °C
195 - 205 °F
Huntsman IROGRAN® A 85 H 4827 TPU-Polyester
Introduction: IROGRAN A 85 H 4827 is a thermoplastic polyester polyurethane for injection molding applications. IROGRAN A 85 H 4827 is part of the HUNTSMAN technical injection molding product range ..