Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 3 | 300 - 320 °C | 572 - 608 °F | |
Lehmann & Voss LUVOCOM® 50/CF/10/GF/10/TF/10/BK Polycarbonate, with carbon fiber, glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Zone 3 | 300 - 320 °C | 572 - 608 °F | |
Lehmann & Voss LUVOCOM® 50/CF/10/TF/15/BK 100 Polycarbonate, with carbon fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Zone 3 | 300 - 320 °C | 572 - 608 °F | |
Lehmann & Voss LUVOCOM® 50/CF/15/TF/15/SI/2/BK Polycarbonate, with carbon fiber, PTFE, lubricant modified Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Zone 3 | 300 - 320 °C | 572 - 608 °F | |
Lehmann & Voss LUVOCOM® 50/CF/20 Polycarbonate, with carbon fiber, low-warpage Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Reduced moment of inertia compared with me.. |
|||
Zone 3 | 300 - 320 °C | 572 - 608 °F | |
Lehmann & Voss LUVOCOM® 50/GF/10/TF/18/SI/2/GY5 Polycarbonate, with glass fiber, PTFE, lubricant modified Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Zone 3 | 300 - 320 °C | 572 - 608 °F | |
Lehmann & Voss LUVOCOM® 50/TF/15/BK-1 Polycarbonate, with PTFE, easy flowing Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
Zone 3 | 300 - 320 °C | 572 - 608 °F | |
Lehmann & Voss LUVOCOM® 50/TF/15/BK7284 Polycarbonate, with PTFE, easy flowing Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
Zone 3 | 300 - 320 °C | 572 - 608 °F | |
Lehmann & Voss LUVOCOM® 50-0828 Polycarbonate, with glass fiber, PTFE, lubricant modified Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Zone 3 | 300 - 320 °C | 572 - 608 °F | |
Lehmann & Voss LUVOCOM® 50-0957 Polycarbonate, with PTFE, easy flowing Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
Zone 3 | 300 - 320 °C | 572 - 608 °F | |
Lehmann & Voss LUVOCOM® 50-1396 Polycarbonate, with carbon fiber, glass fiber and PTFE, electrically conducting Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Zone 3 | 300 - 320 °C | 572 - 608 °F | |
Lehmann & Voss LUVOCOM® 50-7110 Polycarbonate, with carbon fiber, low-warpage, easy flowing Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Electrically conductive, suitable for continuous discharging o.. |
|||
Zone 3 | 300 - 320 °C | 572 - 608 °F | |
Lehmann & Voss LUVOCOM® 50-7216 Polycarbonate, with PTFE, easy flowing Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
Zone 3 | 300 - 320 °C | 572 - 608 °F | |
Lehmann & Voss LUVOCOM® 50-7317 Polycarbonate, with PTFE, easy flowing Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
Zone 3 | 300 - 320 °C | 572 - 608 °F | |
Lehmann & Voss LUVOCOM® 50-7644 Polycarbonate, with carbon fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Electrically conductive, suitable for cont.. |
|||
Zone 3 | 300 - 320 °C | 572 - 608 °F | |
Lehmann & Voss LUVOCOM® 50-7897 Polycarbonate, with PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
Zone 3 | 300 - 320 °C | 572 - 608 °F | |
Lehmann & Voss LUVOCOM® 50-8025 Polycarbonate, with glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Zone 3 | 300 - 320 °C | 572 - 608 °F | |
Lehmann & Voss LUVOCOM® 50-8076 Polycarbonate, with carbon fiber Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High dimensionally stable precision parts with low warpage and.. |
|||
Zone 3 | 300 - 320 °C | 572 - 608 °F | |
Lehmann & Voss LUVOCOM® 50-8479/BL-1 Polycarbonate, unreinforced Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Isotropic shrinkage characteristics.Reduced moment of inertia .. |
|||
Zone 3 | 300 - 320 °C | 572 - 608 °F | |
Lehmann & Voss LUVOCOM® 50/CF/5/GF/10 Polycarbonate, with carbon fiber and glass fiber Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Zone 3 | 300 - 360 °C | 572 - 680 °F | |
Solvay Specialty Polymers Hyflon® MFA® F1520 Perfluoropolymer Hyflon® F is a family of MFA polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame resistance, low s.. |
|||
Zone 3 | 300 - 360 °C | 572 - 680 °F | |
Solvay Specialty Polymers Hyflon® MFA® F1530 Perfluoropolymer Hyflon® MFA is a family of perfluoro polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame resistanc.. |
|||
Zone 3 | 300 °C | 572 °F | Metering-zone |
BASF Ultramid® A3EG10 50% Glass Filled PA66 (Dry) Description: 50% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness as well as for electric insulating parts.Information provided by BASF |
|||
Zone 3 | 300 °C | 572 °F | Metering-zone |
BASF Ultramid® A3W2G10 BK 20560 50% Glass Filled PA66 (Dry) Description: 50% glass fiber reinforced injection molding grade with optimized heat ageing performance for industrial articles having very high rigidity.Information provided by BASF |
|||
Zone 3 | 300 - 320 °C | 572 - 608 °F | |
Lehmann & Voss PLASLUBE J-50/10/TF/15/BK Polycarbonate, with glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High dimensionally stable precision parts, even at elevated te.. |