Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 4 | 196 °C | 385 °F | Extrusion |
Lubrizol ESTANE® 58244 Ether Based Thermoplastic Polyurethane Features: Non-Halogenated flame retardant compoundUses: Extrusion – wire and cable and general extrusion where flame retardant propertied are requiredAvailable in Americas, Europe, Middle East, Afr.. |
|||
Zone 4 | 196 °C | 385 °F | Extrusion |
Lubrizol ESTANE® 58810 Ether Based Thermoplastic Polyurethane Features: High melt flow and improved temperature resistanceUses: Extrusion – Wire and cable, Hose and tubeAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by .. |