Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Zone 5 = 180 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 5 180 °C
356 °F
Borealis Borcell™ HE1123 High Density Polyethylene
Borcell™ HE1123 is a high density polyethylene compound intended for the insulation of radio frequency coaxial cables. Borcell™ HE1123 is designed to give the lowest possible cable attenuation by..
Zone 5 180 °C
356 °F
Blown Film Coextrusion
DuPont™ Appeel® 20D828 Ethylene Acrylate
Appeel® 20D828 is an modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide strong peelable seals over a broad temp..
Zone 5 180 °C
356 °F
Blown Film Coextrusion
DuPont™ Appeel® 20D855 Ethylene Acrylate
DuPont™ Appeel 20D855 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad tempe..
Zone 5 180 °C
356 °F
Blown Film Coextrusion
DuPont™ Appeel® 20D867 Ethylene Acrylate
DuPont™ Appeel 20D867 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad tempe..
Zone 5 180 °C
356 °F
Blown Film Coextrusion
DuPont™ Appeel® 20D875 Ethylene Acrylate
Appeel® 20D875 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide strong peelable seals over a broad tempe..
Zone 5 180 °C
356 °F
Blown Film Coextrusion
DuPont™ Appeel® 22D843 Ethylene Acrylate
DuPont™ Appeel® 22D843 is a polypropylene modified ethylene acrylate resin designed to function as a masterbatch to achieve peelability in polypropylene based sealant layers. It provides peelable ..
Zone 5 180 °C
356 °F
Blown Film Coextrusion
DuPont™ Appeel® 72D727 Sealing Resin
DuPont™ Appeel® 72D727 is a blown or cast film resin designed to be a sealing layer to film or sheet lidding applications. It provides a peelable seal to a number of materials including HDPE, LLDP..
Zone 5 180 °C
356 °F
Blown Film Coextrusion
DuPont™ Appeel® 20D784 Ethylene Acrylate
Appeel® 20D784 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad temperature ..