Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Zone 5 = 230 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 5 230 °C
446 °F
Cylinder
Premix Thermoplastics PRE-ELEC® PE 1200 Conductive Thermoplastic Compound
PRE-ELEC® PE 1200 is a conductive thermoplastic masterbatch/compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. PRE-ELEC® PE 1200 has a high concentration o..
Zone 5 230 °C
446 °F
Cylinder
Premix Thermoplastics PRE-ELEC® PE 1296 Conductive Thermoplastic Compound
PRE-ELEC® PE 1296 is a conductive thermoplastic masterbatch/compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. PRE-ELEC® PE 1296 has a high concentration o..
Zone 5 230 °C
446 °F
Cylinder
Premix Thermoplastics PRE-ELEC® PE 1297 Conductive Thermoplastic Compound
PRE-ELEC® PE 1297 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PE..
Zone 5 230 °C
446 °F
Cylinder
Premix Thermoplastics PRE-ELEC® PE 1299 Conductive Thermoplastic Compound
PRE-ELEC® PE 1299 is a conductive thermoplastic masterbatch/compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. PRE-ELEC® PE 1299 has a high concentration o..
Zone 5 230 °C
446 °F
Die
Premix Thermoplastics PRE-ELEC® PP 1391 Conductive Thermoplastic Compound
PRE-ELEC® PP 1391 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E..
Zone 5 230 °C
446 °F
Cylinder
Premix Thermoplastics PRE-ELEC® PP 1391 Conductive Thermoplastic Compound
PRE-ELEC® PP 1391 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E..
Zone 5 230 °C
446 °F
Die
Premix Thermoplastics PRE-ELEC® PP 1394 Conductive Thermoplastic Compound
PRE-ELEC® PP 1394 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E..
Zone 5 230 °C
446 °F
Cylinder
Premix Thermoplastics PRE-ELEC® PP 1394 Conductive Thermoplastic Compound
PRE-ELEC® PP 1394 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E..
Zone 5 230 °C
446 °F
Die
Premix Thermoplastics PRE-ELEC® PP 1397 Conductive Thermoplastic Compound
PRE-ELEC® PP 1397 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E..
Zone 5 230 °C
446 °F
Cylinder
Premix Thermoplastics PRE-ELEC® PP 1397 Conductive Thermoplastic Compound
PRE-ELEC® PP 1397 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E..
Zone 5 230 °C
446 °F
Injection Molding
UBE UBESTA® 3020GX6 Glass Fiber Reinforced Nylon 12
Description: UBE UBESTA® Automotive grade Nylon 12Comments: conductive, glass fiber reinforced, UV resistanceInformation provided by UBE.
Zone 5 230 °C
446 °F
Injection Molding
UBE UBESTA® 3020GX9 23% Glass Fiber Reinforced Nylon 12
Description: UBE UBESTA® Automotive grade Nylon 12Comments: 23% glass fiber reinforced gradeInformation provided by UBE.
Zone 5 230 °C
446 °F
Injection Molding
UBE UBESTA® 3030LUX Rigid Automotive Grade Nylon 12
Description: UBE UBESTA® Automotive grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE.
Zone 5 230 °C
446 °F
Injection Molding
UBE UBESTA® 3030UFX1 Rigid Industrial Grade Nylon 12
Description: UBE UBESTA® Industrial grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE.
Zone 5 230 °C
446 °F
Injection Molding
UBE UBESTA® 3035UF Rigid Piping Grade Nylon 12
Description: UBESTA contributes to the field of Utilities such as plastic pipe system evolutionary developed for gas industry. It is used for both burial and for rehabilitation of existing cast iron..
Zone 5 230 - 245 °C
446 - 473 °F
Flange
BASF Ultramid® HFX 33 PA6 (Dry)
Description: Ultramid HFX 33 is a polyamide specialty extrusion resin combining high flexibility, excellent burst performance and outstanding chemical resistance. It offers high melt strength and en..
Zone 5 230 - 245 °C
446 - 473 °F
Flange
BASF Ultramid® HFX 35 PA6 (Dry)
Description: Ultramid HFX 35 is a polyamide specialty extrusion resin combining high flexibility, outstanding chemical resistance and enhanced heat stability.Applications: Ultramid HFX 35 is recomme..
Zone 5 230 - 245 °C
446 - 473 °F
Flange
BASF Ultramid® HFX 37 PA6 (Dry)
Description: Ultramid HFX 37 is a polyamide specialty extrusion resin combining high flexibility, excellent burst performance and outstanding chemical resistance. It offers high melt strength and en..
Zone 5 230 °C
446 °F
Injection Molding
UBE UBESTA® 3030LUX 8x1 mm Black Automotive Grade Nylon 12 Tube
Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: rigid, stabilized against weatherability (DIN 73378 Nomenclature = PA12 HL)Information provided by UBE.
Zone 5 230 - 275 °C
446 - 527 °F
Ascend Performance Materials Vydyne® 75HF Nylon 66/6, Heat Stabilized, DAM
Vydyne® 75HF is a medium-high-viscosity, heat-stabilized PA66/6 copolymer resin designed for extrusion applications. It is available in natural color only. Vydyne 75HF resin offers a well-balanced ..
Zone 5 230 - 245 °C
446 - 473 °F
Head
BASF Nypel® 2351 HS BK PA6 (Dry)
Description: Nypel® 2351 HS BK is a heat stabilized, pigmented black, impact modified PA6 extrusion grade compound. Quality and performance are combines at a lower cost. It is based on recycled PA6..
Copyright © lookpolymers.com All Rights Reserved