Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 12600 min @Temperature 16.0 °C |
210 hour @Temperature 60.8 °F |
Full Chemical |
Chesterton ARC PW Potable Water Coating Description: ARC PW is a 100% solids lining certified for NSF/ANSI 61 potable water, cold water service. It is recommended to be applied by brush, roll or spray at 500-750 microns (20-30 mils) total.. |
|||
Cure Time | 12600 min @Temperature 16.0 °C |
210 hour @Temperature 60.8 °F |
Full Chemical |
Chesterton ARC S1 General purpose coating Description: An advanced polymer composite formulated to protect metal surfaces from corrosion and chmical attack. It is normally applied at a thickness of 250 microns (10 mils) per coat. Non-shrink.. |