Polymer Property : Cure Time = 4.02 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time <= 4.02 min

@Temperature 75.0 °C
<= 0.0670 hour

@Temperature 167 °F
touch dry
Gwent Electronic Materials C2021031D2 Electrode Ink
Electrode Ink C2021031D2 is a Silver Palladium (85/15) electrode ink, designed for use with PVB Tape. It has been specifically formulated for use with PZT ceramics.The ink is in a ready to use form..
Cure Time <= 4.02 min

@Temperature 75.0 °C
<= 0.0670 hour

@Temperature 167 °F
touch dry
Gwent Electronic Materials C2021031D3 Electrode Ink
Electrode Ink C2021031D3 is a Silver Palladium (90/10) electrode ink, designed for use with PVB Tape. It has been specifically formulated for use with PZT ceramics.The ink is in a ready to use form..
Cure Time 4.02 min

@Temperature 75.0 °C
0.0670 hour

@Temperature 167 °F
Dust Free, at 50% humidity
Blue River Coatings Steel Seal Primer
BLUE RIVER COATINGS STEEL SEAL PRIMER is a high quality, single component primer, not requiring any catalyzing agent. STEEL SEAL PRIMER is designed for dip coaters who need a quick, fast drying pain..
Cure Time 4.02 - 4.98 min

@Temperature 75.0 °C
0.0670 - 0.0830 hour

@Temperature 167 °F
Recoat, at 50% humidity
Blue River Coatings Steel Seal Primer
BLUE RIVER COATINGS STEEL SEAL PRIMER is a high quality, single component primer, not requiring any catalyzing agent. STEEL SEAL PRIMER is designed for dip coaters who need a quick, fast drying pain..