Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 3.00 - 4.98 min @Temperature 75.0 °C |
0.0500 - 0.0830 hour @Temperature 167 °F |
Recoat, at 50% humidity |
Blue River Coatings Acrylic 4000D Topcoat BLUE RIVER COATINGS ACRYLIC 4000 TOPCOAT is a hard, flexible, economical coating designed for multiple substrates. BLUE RIVER COATINGS ACRYLIC 4000 TOPCOAT offers good application properties, low fo.. |
|||
Cure Time | 4.02 - 4.98 min @Temperature 75.0 °C |
0.0670 - 0.0830 hour @Temperature 167 °F |
Recoat, at 50% humidity |
Blue River Coatings Steel Seal Primer BLUE RIVER COATINGS STEEL SEAL PRIMER is a high quality, single component primer, not requiring any catalyzing agent. STEEL SEAL PRIMER is designed for dip coaters who need a quick, fast drying pain.. |
|||
Cure Time | 3.00 - 4.98 min @Temperature 75.0 °C |
0.0500 - 0.0830 hour @Temperature 167 °F |
Recoat, at 50% humidity |
Blue River Coatings Acrylic 4000 Topcoat BLUE RIVER COATINGS ACRYLIC 4000 TOPCOAT is a hard, flexible, economical coating designed for multiple substrates. BLUE RIVER COATINGS ACRYLIC 4000 TOPCOAT offers good application properties, low fo.. |