Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 360 - 480 min @Temperature 25.0 °C |
6.00 - 8.00 hour @Temperature 77.0 °F |
De-mold Time |
Northstar Polymers MPP-A47A Liquid Castable Polyurethane MPP-A47A is a room-temperature-cure liquid castable polyurethane system. This ether-base polyurethane system is used in applications such as mold-making, prototyping, production of cast parts, pott.. |
|||
Cure Time | 300 - 480 min @Temperature 25.0 °C |
5.00 - 8.00 hour @Temperature 77.0 °F |
De-mold Time |
Northstar Polymers MPG-A25A Room-Temperature Curable Liquid Castable Polyurethane MPG-A25A is a room-temperature-cure liquid castable polyurethane system. This ether-base polyurethane system is used in applications such as mold-making, prototyping, production of cast parts, pott.. |
|||
Cure Time | 360 - 480 min @Temperature 23.9 °C |
6.00 - 8.00 hour @Temperature 75.0 °F |
for 48 hrs, plus 140-150°F |
Master Bond Super Gel 9AO Thermally Conductive Urethane Modified Epoxy Gel Description: Master Bond Super Gel 9AO is a two component, urethane modified epoxy system that cures at room temperature with softness and dimensional stability. Additionally, it possesses good ther.. |
|||
Cure Time | 360 - 480 min @Temperature 23.9 °C |
6.00 - 8.00 hour @Temperature 75.0 °F |
for 48 hrs, plus 140-150°F |
Master Bond Super Gel 9AOND Dimensionally Stable Urethane Modified Epoxy Master Bond Super Gel 9AOND is a two component, urethane modified epoxy system that cures at room temperature and has a paste-like consistency. It offers softness and retains dimensional stability. .. |
|||
Cure Time | 360 - 480 min @Temperature 24.0 °C |
6.00 - 8.00 hour @Temperature 75.2 °F |
demold time |
BCC Products BC 8160 Urethane Casting BC8160 is a low viscosity two-component urethane casting compound that is specifically formulated for its flexural and impact strength. It is recommended for use for the production casting of highly.. |
|||
Cure Time | 360 - 480 min @Temperature 24.0 °C |
6.00 - 8.00 hour @Temperature 75.2 °F |
demold time |
BCC Products BC 8782 Urethane Casting BC 8782 produces a high impact rigid 82 Shore D material that is commonly used to make clear or tinted castings of all kinds. When used at room temperature castings 1/8" thick or larger can be readi.. |