Processing Properties | Metric | English | Comments |
---|---|---|---|
Sintering Temperature | >= 850 °C | >= 1560 °F | For at least 10 mins |
Gwent Electronic Materials C2000904P3 Platinum Ink It can be used on partially stabilized zirconia and tape cast Materials. The Platinum powder contained within this paste has low shrinkage and high adhesion to ceramic substrates. Screen Printing E.. |
|||
Sintering Temperature | 850 - 1150 °C | 1560 - 2100 °F | |
Gwent Electronic Materials C2050830D8 80:20 Silver Palladium Ink C2050830D8 is an ink based on a 80:20 ratio of Silver:Palladium. It is designed for use in Single Layer PZT applications. This ink can be used in both dip and hand soldering. This Ink is in a ready .. |
|||
Sintering Temperature | 850 - 1150 °C | 1560 - 2100 °F | |
Gwent Electronic Materials C2050905D3 80:20 Silver Palladium Ink C2050905D3 is an ink based on a 80:20 ratio of Silver:Palladium; a screen printing internal electrode ink for flexible PZT components. This Material is compatible with PVB tape. The ink is designed .. |
|||
Sintering Temperature | 850 - 1150 °C | 1560 - 2100 °F | |
Gwent Electronic Materials C2090512D1 70:30 Silver Palladium Ink C2090512D1 is an ink based on a 70:30 ratio of Silver:Palladium. It is designed as an internal electrode ink for use with PVB tape. Screen Printing Equipment: semi-automatic, manualScreen Types: sta.. |
|||
Sintering Temperature | >= 850 °C | >= 1560 °F | non-oxygen and reducing atmosphere |
Gwent Electronic Materials C2100419D1 Copper Paste This product has been designed as a copper ink for use in termination and circuit printing on ceramic substrates. This product contains a glass frit so may not be suitable for internal electrodes. .. |
|||
Sintering Temperature | >= 850 °C | >= 1560 °F | |
Gwent Electronic Materials D2020409D8 Dielectric for Stainless Steel Dielectric is suitable for use as an insulation layer when printed and fired on to stainless steel. The thermal coefficient of expansion of this product has been matched to that of stainless steel. .. |
|||
Sintering Temperature | 850 - 1150 °C | 1560 - 2100 °F | |
Gwent Electronic Materials C2090615D1 70:30 Silver Palladium Ink C2090615D1 is an ink based on a 70:30 ratio of Silver:Palladium. It is designed as an internal electrode ink. Screen Printing Equipment: semi-automatic, manualScreen Types: stainless steel, polyeste.. |
|||
Sintering Temperature | >= 850 °C | >= 1560 °F | Reducing atmosphere |
Gwent Electronic Materials C2100316D1 Nickel Ink This product has been designed as a nickel ink for use in internal electrodes and for use with Solid Oxide Fuel Cells. This electrode ink is designed for use with ML Ceramic Tapes. The ink should .. |