Polymer Property : Sintering Temperature = 2100 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Sintering Temperature 850 - 1150 °C
1560 - 2100 °F
Gwent Electronic Materials C2050830D8 80:20 Silver Palladium Ink
C2050830D8 is an ink based on a 80:20 ratio of Silver:Palladium. It is designed for use in Single Layer PZT applications. This ink can be used in both dip and hand soldering. This Ink is in a ready ..
Sintering Temperature 850 - 1150 °C
1560 - 2100 °F
Gwent Electronic Materials C2050905D3 80:20 Silver Palladium Ink
C2050905D3 is an ink based on a 80:20 ratio of Silver:Palladium; a screen printing internal electrode ink for flexible PZT components. This Material is compatible with PVB tape. The ink is designed ..
Sintering Temperature 850 - 1150 °C
1560 - 2100 °F
Gwent Electronic Materials C2090512D1 70:30 Silver Palladium Ink
C2090512D1 is an ink based on a 70:30 ratio of Silver:Palladium. It is designed as an internal electrode ink for use with PVB tape. Screen Printing Equipment: semi-automatic, manualScreen Types: sta..
Sintering Temperature 850 - 1150 °C
1560 - 2100 °F
Gwent Electronic Materials C2090615D1 70:30 Silver Palladium Ink
C2090615D1 is an ink based on a 70:30 ratio of Silver:Palladium. It is designed as an internal electrode ink. Screen Printing Equipment: semi-automatic, manualScreen Types: stainless steel, polyeste..