Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Sintering Temperature = 1650 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Sintering Temperature 900 °C

@Time 7200 sec
1650 °F

@Time 2.00 hour
PPT LSF120 Low Sintering Temperature Ferrite Powder
Uses: Low Temperature Co-fired Ceramic Components (LTCC), Multi-Layer Chip Inductors (MLCI), Chip Beads (EMI Suppressors)Electromagnetic proerties reported were tested on sintered toroids with a HP4..
Sintering Temperature 900 °C

@Time 7200 sec
1650 °F

@Time 2.00 hour
PPT LSF16 Low Sintering Temperature Ferrite Powder
Uses: Low Temperature Co-fired Ceramic Components (LTCC), Multi-Layer Chip Inductors (MLCI), Chip Beads (EMI Suppressors)Electromagnetic proerties reported were tested on sintered toroids with a HP4..
Sintering Temperature 900 °C

@Time 7200 sec
1650 °F

@Time 2.00 hour
PPT LSF180 Low Sintering Temperature Ferrite Powder
Uses: Low Temperature Co-fired Ceramic Components (LTCC), Multi-Layer Chip Inductors (MLCI), Chip Beads (EMI Suppressors)Electromagnetic proerties reported were tested on sintered toroids with a HP4..
Sintering Temperature 900 °C

@Time 7200 sec
1650 °F

@Time 2.00 hour
PPT LSF220 Low Sintering Temperature Ferrite Powder
Uses: Low Temperature Co-fired Ceramic Components (LTCC), Multi-Layer Chip Inductors (MLCI), Chip Beads (EMI Suppressors)Electromagnetic proerties reported were tested on sintered toroids with a HP4..
Sintering Temperature 900 °C

@Time 7200 sec
1650 °F

@Time 2.00 hour
PPT LSF25 Low Sintering Temperature Ferrite Powder
Uses: Low Temperature Co-fired Ceramic Components (LTCC), Multi-Layer Chip Inductors (MLCI), Chip Beads (EMI Suppressors)Electromagnetic proerties reported were tested on sintered toroids with a HP4..
Sintering Temperature 900 °C

@Time 7200 sec
1650 °F

@Time 2.00 hour
PPT LSF400 Low Sintering Temperature Ferrite Powder
Uses: Low Temperature Co-fired Ceramic Components (LTCC), Multi-Layer Chip Inductors (MLCI), Chip Beads (EMI Suppressors)Electromagnetic proerties reported were tested on sintered toroids with a HP4..
Sintering Temperature 900 °C

@Time 7200 sec
1650 °F

@Time 2.00 hour
PPT LSF50 Low Sintering Temperature Ferrite Powder
Uses: Low Temperature Co-fired Ceramic Components (LTCC), Multi-Layer Chip Inductors (MLCI), Chip Beads (EMI Suppressors)Electromagnetic proerties reported were tested on sintered toroids with a HP4..