Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 166 - 188 °C | 331 - 370 °F | |
PolyOne Dynaflex™ D3202-1000-03 Thermoplastic Elastomer (TPE) Dynaflex™ D3202-1000-03 is an easy processing TPE designed for general purpose applications and is suitable for injection molding, extrusion, blow molding, and thermoforming processes. - Dry Feel -.. |
|||
Middle Barrel Temperature | 166 - 188 °C | 331 - 370 °F | |
PolyOne Dynaflex™ D3204-1000-03 Thermoplastic Elastomer (TPE) Dynaflex™ D3204-1000-03 is an easy processing TPE designed for general purpose applications and is suitable for injection molding, extrusion, blow molding, and thermoforming processes. - Dry Feel -.. |
|||
Middle Barrel Temperature | 166 - 188 °C | 331 - 370 °F | |
PolyOne Dynalloy™ OBC8000-T05 Thermoplastic Elastomer (TPE) Dynalloy™ OBC8000-T05 is an ultra-soft TPE utilizing the unique rubber properties of Dows INFUSE™ Olefin Block Copolymers. This product is designed for injection molding applications where excepti.. |
|||
Middle Barrel Temperature | 166 - 171 °C | 330 - 340 °F | |
Kleerdex Kydex® P55 Acrylic/PVC Extrusion Compound
(discontinued **) Weatherable profile extrusion compoundApplications: Extruded profiles requiring weatherability, high flexural modulus, and excellent flammability resistance. Features: Weatherability is dependent o.. |
|||
Middle Barrel Temperature | 166 - 193 °C | 330 - 380 °F | |
Clariant CA9000NAT` Acetal Copolymer Data provided by Clariant Masterbatches |