Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 170 - 180 °C | 338 - 356 °F | |
Multibase TPSiV® 4100-70A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Low compression setAPPLICATIONS: Solution for soft touch overmolding on consumer electr.. |
|||
Middle Barrel Temperature | 170 - 180 °C | 338 - 356 °F | |
Multibase TPSiV® 4200-60A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Good chemical resistanceAPPLICATIONS: Solution for soft touch overmolding on consumer e.. |
|||
Middle Barrel Temperature | 170 - 180 °C | 338 - 356 °F | |
Multibase TPSiV® 4200-70A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Good chemical resistanceAPPLICATIONS: Solution for soft touch overmolding on consumer e.. |
|||
Middle Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Start Point: 180°C |
Kingfa HF-618 Flame Retardant ABS Features:UL 94 V-0 @ 1.6-3.0mmHigh toughnessEasy flowApplications:Injection moldingShell of applianceCD-ROMPower switchInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Middle Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Injection Molding |
LG Chemical LUCEL FW700N Modified POM, Friction Resistance, Abrasion Resistance Feature: Injection Molding, Modified POM, Friction Resistance, Abrasion ResistanceApplication: Gears, Printer Roller Pumps, Gear Worm WheelsCAS No. 66455-31-0Information provided by LG Chemical |
|||
Middle Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Injection Molding |
LG Chemical LUCEL FW700S Modified POM, Friction Resistance, Abrasion Resistance Feature: Injection Molding, Modified POM, Friction Resistance, Abrasion ResistanceApplication: Gears, Printer Roller Pumps, Gear Worm WheelsCAS No. 66455-31-0Information provided by LG Chemical |
|||
Middle Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Injection Molding |
LG Chemical LUCEL HI510 POM+Rubber, High Impact Feature: Injection Molding, POM+Rubber, High ImpactApplication: Gears, Automobile ClipCAS No. 66455-31-0Information provided by LG Chemical |
|||
Middle Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Injection Molding |
LG Chemical LUCEL HI520 POM+Rubber, High Impact Feature: Injection Molding, POM+Rubber, High ImpactApplication: GearsCAS No. 66455-31-0 and 155123-66-3Information provided by LG Chemical |
|||
Middle Barrel Temperature | 170 - 175 °C | 338 - 347 °F | |
Metabolix Mirel™ F1006 Injection Molding Grade PHA Bioplastic Mirel F1006 is FDA cleared for use in non-alcoholic food contact applications, from frozen food storage and microwave reheating to boiling water up to 212°F. FDA clearance includes products such.. |
|||
Middle Barrel Temperature | 170 - 175 °C | 338 - 347 °F | |
Metabolix Mirelâ„¢ P1004 Injection Molding Grade PHA Bioplastic Mirel P1004 is a general purpose injection molding grade with high toughness.About Mirel BioplasticsMirel is a family of bioplastic materials that have physical properties comparable to petroleum-ba.. |
|||
Middle Barrel Temperature | 170 °C | 338 °F | Compress zone |
Taiwan PU Corporation TPU-C75 General Grade, Calender Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Calender MoldingInformation provided by Taiwan PU Corporation. |
|||
Middle Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Injection Molding |
Stellarchem SV-B65E TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Middle Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Injection Molding |
Stellarchem SV-B70E TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Middle Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Injection Molding |
Stellarchem SV-B80E TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Middle Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Injection Molding |
Stellarchem SV-B87E TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Middle Barrel Temperature | 170 °C | 338 °F | |
SK Chemicals SKYTHANE® T870A Polyester Based, Low Hardness Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Middle Barrel Temperature | 170 - 220 °C | 338 - 428 °F | |
Sumitomo Chemical ESPOLEX® 4785 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Middle Barrel Temperature | 170 - 220 °C | 338 - 428 °F | |
Sumitomo Chemical ESPOLEX® 817 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Middle Barrel Temperature | 170 - 220 °C | 338 - 428 °F | |
Sumitomo Chemical ESPOLEX® 820 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Middle Barrel Temperature | 170 - 220 °C | 338 - 428 °F | |
Sumitomo Chemical ESPOLEX® 822 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Middle Barrel Temperature | 170 - 200 °C | 338 - 392 °F | |
Sumitomo Chemical ESPOLEX® WT315 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Middle Barrel Temperature | 170 - 220 °C | 338 - 428 °F | |
Sumitomo Chemical ESPOLEX® WT525 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Middle Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Mid-2. Region Temperature |
Tisan TISETILEN® Flame Retardant (V0) Polyethylene TISETILEN has a wide area of application in construction, building auxiliary materials, lighting equipment, household appliance, toy industries, etc. General specifications include Low densityFlexib.. |
|||
Middle Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Mid-2. Region Temperature |
Tisan TISETILEN® UNR Polyethylene TISETILEN has a wide area of application in construction, building auxiliary materials, lighting equipment, household appliance, toy industries, etc. General specifications include Low densityFlexib.. |
|||
Middle Barrel Temperature | >= 170 °C | >= 338 °F | |
Borealis Visico™ ME4425/LE4437 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Insulation Visico ME4425/LE4437 is a natural, moisture-induced crosslinking polyethylene compound that is designed for use as low voltage wire insulation and jacketing. ME4425 is a medium-density ethylene vin.. |
|||
Middle Barrel Temperature | 170 - 200 °C | 338 - 392 °F | |
Elastron® V TPV Elastomer Characteristicswide hardness rangedoes not require vulcanisation-quite higher saving on the processing costsremains flexible at low temperatureshigh temperature resistanceelectrical insulator with v.. |