Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical ALPHALAC SG970 HIPS Description: Injection Molding, General Purpose, Good Processability, High glossApplication: Air Conditioner Panel, Washer CoverCAS No. 9003-55-8Information provided by LG Chemical |
|||
Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical GPPS 20HR(E) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: PSP, Food Tray, Electric/Electrical Component, CoatingCAS: 9003-53-6Information provided by LG Chemical |
|||
Middle Barrel Temperature | 190 - 200 °C | 374 - 392 °F | Injection Molding |
LG Chemical HIPS 405AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 158725-44-1 and 1309-64-4Information provided by LG Chemical |
|||
Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical HIPS MI730 PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical KEYFLEX BT 10288D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |
|||
Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | |
LG Chemical LUCEL FW-710F Friction and Wear Resistant POM, PTEE filled LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | |
LG Chemical LUCEL FW-715C Friction and Wear Resistant POM, Polymeric Wear Additive, CaCo3 Filled, Low Warpage, Antistatic LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | |
LG Chemical LUCEL N109-AS Antistatic POM, Unreinforced, Standard Viscosity LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | |
LG Chemical LUCEL N109-HR Heat Resistant POM, Unreinforced, Standard Viscosity LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical LUCEL N109LDS POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | |
LG Chemical LUCEL N127-02 General Purpose POM, Unreinforced, Externally Lubricated, High Flow LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Middle Barrel Temperature | 190 - 200 °C | 374 - 392 °F | |
Huntsman AVALON® 92 AE Thermoplastic Polyurethane Introduction: AVALON 92 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 92 AE is part of the AVALON Perform Range and offers a premium soiling materi.. |
|||
Middle Barrel Temperature | 190 - 200 °C | 374 - 392 °F | |
Huntsman AVALON® 95 AE Thermoplastic Polyurethane Introduction: AVALON 95 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 95 AE is part of the AVALON Perform Range and offers a premium soiling materi.. |
|||
Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical 80HF SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical |
|||
Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Transition, Extrusion |
Stellarchem AB760LG TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Transition, Extrusion |
Stellarchem AB855LG TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
Stellarchem AB870LG TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Transition, Extrusion |
Stellarchem AB870LG TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Transition, Extrusion |
Stellarchem FP-860 TPE Compound Product description : This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric poly.. |
|||
Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
Stellarchem GP-9401 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
Stellarchem GP-965B TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Transition, Extrusion |
Stellarchem GP-965B TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
Stellarchem GP-975 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
Stellarchem HP-930NC-HD TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
Stellarchem MP-8001 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Transition, Extrusion |
Stellarchem MP-8001 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Transition, Extrusion |
Stellarchem MP-850 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Middle Barrel Temperature | 170 - 200 °C | 338 - 392 °F | |
Sumitomo Chemical ESPOLEX® WT318 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | |
Unitika TERRAMAC TE-7000 Polylactic Acid (PLA) Heat-resisting grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical KEYFLEX BT 1035D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |