Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 204 - 216 °C | 400 - 420 °F | |
PlastiComp Complet® LCF30 - PP Homopolymer Polypropylene, 30% Long Carbon Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 30% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Middle Barrel Temperature | 204 - 216 °C | 400 - 420 °F | |
PlastiComp Complet® LCF50 - PP Homopolymer Polypropylene, 50% Long Carbon Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 50% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Middle Barrel Temperature | 204 - 216 °C | 400 - 420 °F | |
PlastiComp Complet® LGF20 - PP Homopolymer Polypropylene, 20% Long Glass Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 20% long glass fiber reinforcementInformation provided by PlastiComp, In.. |
|||
Middle Barrel Temperature | 204 - 216 °C | 400 - 420 °F | |
PlastiComp Complet® LGF50 - PP Homopolymer Polypropylene, 50% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 50% long glass fiber reinforcementInformation provided by PlastiCom.. |
|||
Middle Barrel Temperature | 193 - 216 °C | 379 - 421 °F | |
PolyOne Versaflex™ HC 2110-57B Thermoplastic Elastomer (TPE) Versaflex™ HC 2110-57B is a TPE designed for use in the healthcare industry offering low stiction and good compression set. New Product. Commercial specifications have not been established. - Bonds.. |
|||
Middle Barrel Temperature | 177 - 216 °C | 351 - 421 °F | |
PolyOne Dynaflex™ G7410-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7410-1000-00 is an easy processing, high performance compound designed for use in applications requiring a tough, durable material. - Excellent Colorability - Excellent Heat Stability - .. |
|||
Middle Barrel Temperature | 193 - 216 °C | 380 - 420 °F | |
MRC Polymers MAXTELâ„¢ 600T25 TPO, 25% Talc Filled For automotive exterior applicationsExcellent process ability and dimensional stabilityCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Polymers Inc. |
|||
Middle Barrel Temperature | 193 - 216 °C | 380 - 420 °F | |
MRC Polymers MAXTELâ„¢ 600T30IM TPO, 30% Talc Filled For automotive exterior applicationsExcellent process ability and dimensional stabilityImpact ModifiedCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Pol.. |
|||
Middle Barrel Temperature | 193 - 216 °C | 380 - 420 °F | |
MRC Polymers MAXTELâ„¢ 600-BK TPO, Black For automotive exterior applications. Excellent process ability and dimensional stability.Unfilled TPOAvailable in black and gray onlyCan be UV StabilizedInternal and external lubricants can be add.. |
|||
Middle Barrel Temperature | 177 - 216 °C | 350 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 3135 Thermoplastic Elastomer A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3135 can be processed by injection molding or extrusion for ap.. |
|||
Middle Barrel Temperature | 177 - 216 °C | 350 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 3190 Thermoplastic Elastomer A medium hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3190 can be processed by blow molding, injection molding or.. |
|||
Middle Barrel Temperature | 177 - 216 °C | 350 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 3439D Thermoplastic Elastomer A NSF certified, high hardness, multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by injectio.. |
|||
Middle Barrel Temperature | 177 - 216 °C | 350 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 3440 Thermoplastic Elastomer A NSF certified, low hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inject.. |
|||
Middle Barrel Temperature | 177 - 216 °C | 350 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 3450 Thermoplastic Elastomer A NSF certified, low hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inject.. |
|||
Middle Barrel Temperature | 177 - 216 °C | 350 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 3470 Thermoplastic Elastomer A NSF certified, medium hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inj.. |
|||
Middle Barrel Temperature | 177 - 216 °C | 350 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 3490N Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |
|||
Middle Barrel Temperature | 177 - 216 °C | 350 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 4145 Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4145 is a low hardness grade possessing exceptional tensile strength, superior compression set, chemical re.. |
|||
Middle Barrel Temperature | 177 - 216 °C | 350 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 4180 Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4180 is a medium hardness grade possessing exceptional tensile strength, superior compression set, chemical.. |
|||
Middle Barrel Temperature | 177 - 216 °C | 350 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 4445 Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4445 is a low hardness grade possessing exceptional tensile strength, superior compression s.. |
|||
Middle Barrel Temperature | 177 - 216 °C | 350 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 4455 Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4455 is a low hardness grade possessing exceptional tensile strength, superior compression s.. |
|||
Middle Barrel Temperature | 177 - 216 °C | 350 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 4465 Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4465 is a low hardness grade possessing exceptional tensile strength, superior compression s.. |
|||
Middle Barrel Temperature | 177 - 216 °C | 350 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 3460N Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |
|||
Middle Barrel Temperature | 177 - 216 °C | 350 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 3480 Thermoplastic Elastomer A NSF certified, medium hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inj.. |
|||
Middle Barrel Temperature | 177 - 216 °C | 350 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 3490 Thermoplastic Elastomer A NSF certified, medium hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inj.. |
|||
Middle Barrel Temperature | 177 - 216 °C | 350 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 4439D Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4439D is a high hardness grade possessing exceptional tensile strength, superior compression s.. |
|||
Middle Barrel Temperature | 193 - 216 °C | 379 - 421 °F | |
Ineos Nova 8048 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Improved toughness, Custom colorsApplications: Designed for injection molding applications requiring clarity and toughnessPerformance grades of polystyrene are engineered to have specific properties.. |
|||
Middle Barrel Temperature | 193 - 216 °C | 379 - 421 °F | |
Ineos Nova 817 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High flow crystal polystyrene, Custom colorsApplications: Injection molding, Designed for use in high speed, Thin section applications and complex parts designs where custom coloring is a requiremen.. |
|||
Middle Barrel Temperature | 177 - 216 °C | 350 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 3150 Thermoplastic Elastomer A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3150 can be processed by injection molding or extrusion for appl.. |
|||
Middle Barrel Temperature | 177 - 216 °C | 350 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 3439DN Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |
|||
Middle Barrel Temperature | 177 - 216 °C | 350 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 4149D Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4149D is a high hardness grade possessing exceptional tensile strength, superior compression set, chemical re.. |