Polymer Property : Middle Barrel Temperature = 224 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Middle Barrel Temperature 224 - 235 °C
435 - 455 °F
PTS PCA-1010HF High Flow Polycarbonate/ABS Alloy
Information provided by Polymer Technology and Services, LLC (PTS).
Middle Barrel Temperature 224 - 235 °C
435 - 455 °F
PTS PCA-1011 High Impact Polycarbonate/ABS Alloy
Information provided by Polymer Technology and Services, LLC (PTS).
Middle Barrel Temperature 224 - 235 °C
435 - 455 °F
PTS PCA-1012 High Impact Polycarbonate/ABS Alloy
Information provided by Polymer Technology and Services, LLC (PTS).
Middle Barrel Temperature 224 - 241 °C
435 - 466 °F
A. Schulman ComAlloy Comtuf® 420 Polyester - PBT, High Impact Modified
Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc..