Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman ComAlloy Comtuf® 420 Polyester - PBT, High Impact Modified

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Impact Grade
Manufacturer A. Schulman ComAlloy
Trade Name COMTUF®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman ComAlloy Comtuf® 420 Polyester - PBT, High Impact Modified.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Density 1.26 g/cc
0.0455 lb/in³
Linear Mold Shrinkage 0.018 cm/cm
0.018 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 107
107
ASTM D785
Tensile Strength, Ultimate 28.0 MPa
4060 psi
ASTM D638
Elongation at Break 34.2 %
34.2 %
ASTM D638
Flexural Strength 61.0 MPa
8850 psi
ASTM D790
Flexural Modulus 1.70 GPa
247 ksi
ASTM D790
Izod Impact, Notched 8.11 J/cm
15.2 ft-lb/in
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D256
Thermal Properties Metric English Comments
Melting Point 210 - 225 °C
410 - 437 °F
Deflection Temperature at 0.46 MPa (66 psi) 154 °C
309 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 56.0 °C
133 °F
ASTM D648
Processing Properties Metric English Comments
Middle Barrel Temperature 224 - 241 °C
435 - 466 °F