Polymer Property : Middle Barrel Temperature = 296 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Middle Barrel Temperature 296 - 304 °C
565 - 579 °F
A. Schulman ComAlloy Hiloy® 441 Glass Reinforced, PET Alloy
Data provided by the manufacturer, ComAlloy International Company.33% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 296 - 304 °C
565 - 579 °F
A. Schulman ComAlloy Hiloy® 442 Glass Reinforced, PET Alloy
Data provided by the manufacturer, ComAlloy International Company.45% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 296 - 304 °C
565 - 579 °F
A. Schulman ComAlloy Hiloy® 443 Glass Reinforced, PET Alloy
Data provided by the manufacturer, ComAlloy International Company.55% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 296 - 304 °C
565 - 579 °F
A. Schulman ComAlloy Hiloy® 446 Glass/Mineral Reinforced, PET Alloy
Data provided by the manufacturer, ComAlloy International Company.35% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 296 - 304 °C
565 - 579 °F
A. Schulman ComAlloy Hiloy® 464 Glass Fiber/Bead Reinforced, PET Alloy
Data provided by the manufacturer, ComAlloy International Company.25% Glass Fiber/Bead Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 296 - 304 °C
565 - 579 °F
A. Schulman ComAlloy Voloy® 431 Glass/Mineral Reinforced, PET Alloy, Flame Retardant, UL
Data provided by the manufacturer, ComAlloy International Company.40% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 296 - 304 °C
565 - 579 °F
A. Schulman ComAlloy Voloy® 441 Glass Reinforced, PET Alloy, Flame Retardant, UL
Data provided by the manufacturer, ComAlloy International Company.32% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 296 - 304 °C
565 - 579 °F
A. Schulman ComAlloy Comtuf® 462 Glass/Mineral Reinforced, PET Alloy, Impact Modified, UL
Data provided by the manufacturer, ComAlloy International Company.50% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Copyright © lookpolymers.com All Rights Reserved