Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products F4900-611UV Thermoplastic Polyolefin, UV Stabilized, XS9 Dark Neutral Metallic Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT4802-690UVA Thermoplastic Polyolefin, UV Stabilized, HS5 Medium Dark Neutral Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT4900-33UV Thermoplastic Polyolefin, UV Stabilized, KSD Charcoal Argent Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products G10UP100-01 10% Glass Fiber Reinforced Polypropylene, Black, UL94-HB Rated Applications: Consumer housingsConsumer goodsFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products G13P100-00UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, Natural Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products G13P100-589UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, (YR169L) Mild Beige Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products G13P100-598UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, (NH-293L) Seagull Gray Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products G13P100-724UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, NH220L Clear Gray Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products GC10P100-01 10% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black Applications: Air ducts - distributionFuel filler pocketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products HP514-394 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 102E Medium Oak Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products HP514-489 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 101E Lite Oak Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products HP521-186 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 7701 Graphite Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products HP521-229 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 195A Medium Neutral Applications: Interior trimIP structural componentsScuff/kick platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products T15P100-00 12% Talc Reinforced Polypropylene, Natural Applications: Component housingConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Oxford Polymers ABS 30GF-BK ABS, 30% Glass Fiber Reinforced Product Description: Glass Fiber (30% Reinforced), ABS injection molding grade Processing and Delivery Form: Pellets and Injection Molding Additives: Release AgentsSpecial Characteristics: Pre-colo.. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products HP514-00 14% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® J-60/10/FR Polypropylene Homopolymer, 10% Glass Reinforced, Flame Retardant Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® J-60/20/FR Polypropylene Homopolymer, 20% Glass Reinforced, Flame Retardant Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® J-60/30/E/M Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® J-60/40/E8 Polypropylene Homopolymer, 40% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® PP-61/CC/20 Polypropylene Copolymer, 20% Calcium Carbonate Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 193 - 227 °C | 380 - 440 °F | |
CTC SunPro® SP 200 P3081 Polypropylene Copolymer SunPro® SP 200 P 3081 is a general purpose, medium flow, polypropylene copolymer. It has applications in automotive wheel housings and general purpose automotive. Automotive Certifications: GM PP .. |
|||
Middle Barrel Temperature | 193 - 227 °C | 380 - 440 °F | |
CTC X-PRO CTC PP 2015 Polypropylene Impact Copolymer X-PRO PP 2015 is an impact, polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC). |
|||
Middle Barrel Temperature | 193 - 227 °C | 380 - 440 °F | |
CTC X-PRO CTC PP 2019 Polypropylene Impact Copolymer X-PRO PP 2019 is a high impact, polypropylene copolymer. It has automotive and industrial general purpose applications.Data provided by Composite Technologies (CTC). |
|||
Middle Barrel Temperature | 193 - 227 °C | 380 - 440 °F | |
CTC X-PRO CTC PP 2025 Polypropylene Impact Copolymer X-PRO PP 2025 is an impact, polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC). |
|||
Middle Barrel Temperature | 193 - 227 °C | 380 - 440 °F | |
CTC X-PRO CTC PP 4025 Polypropylene Copolymer X-PRO PP 4025 is a high value polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC). |
|||
Middle Barrel Temperature | 193 - 227 °C | 380 - 440 °F | |
CTC X-PRO CTC PP 5002 Polypropylene Copolymer X-PRO PP 5002 is a polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC). |
|||
Middle Barrel Temperature | 216 - 227 °C | 420 - 440 °F | |
CTC X-PRO TF 1140 HP Polypropylene Homopolymer, 40% Talc Filled X-PRO TF 1140 HP is a 40% talc reinforced polypropylene homopolymer, heat stabilized, and made of 98% recycled content. It has applications in: automotive under hood, IP components, HVAC, and lawn .. |
|||
Middle Barrel Temperature | 216 - 227 °C | 420 - 440 °F | |
Advanced Polymer Alloys DuraGrip™ 6160 BK Melt Processable Elastomer DuraGrip™ 6160BK is designed to be a special purpose Melt Processable Elastomer (MPE) that is easy to use in injection molding and extrusion processes. DGR 6160BK has an excellent
soft touch feel a.. |
|||
Middle Barrel Temperature | 193 - 227 °C | 380 - 440 °F | |
LTL Color Compounds ColorFast® FRPS100 Styrene, High Impact V1-rated high impact styreneAll information provided by LTL Color Compounders, Inc. |