Polymer Property : Front Barrel Temperature = 193 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Front Barrel Temperature 182 - 193 °C
360 - 380 °F
Ravago Manufacturing Americas Hylac® FR134G10 ABS, 10% Glass Fiber Reinforced
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Front Barrel Temperature 177 - 193 °C
350 - 380 °F
Teknor Apex Flexalloy® 9100-65 Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, General Purpose, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather..
Front Barrel Temperature 177 - 193 °C
350 - 380 °F
Teknor Apex Flexalloy® 9300-60 Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, Oil Resistant, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather R..
Front Barrel Temperature 188 - 193 °C
370 - 380 °F
Clariant OMAN698583 Thermoplastic Polyurethane, Halogen Free, Flame Retardant
Aromatic Polyether BasedData provided by Clariant Masterbatches