Material Notes:
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, Oil Resistant, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather ResistanceUses- Automotive Applications, TubingForms-PelletsProcessing-Extrusion, Injection MoldingInformation provided by Teknor Apex Company
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
23°C; ASTM D792
Linear Mold Shrinkage 0.010 - 0.025 cm/cm
0.010 - 0.025 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
15 seconds; ASTM D2240
Tensile Strength, Yield 4.69 MPa
680 psi
100%; ASTM D412
14.8 MPa
2150 psi
ASTM D412
Elongation at Break 340 %
340 %
ASTM D412
Compression Set 32 %
32 %
73°F; ASTM D395
Thermal Properties Metric English Comments
Brittleness Temperature -43.0 °C
-45.4 °F
ASTM D746
Processing Properties Metric English Comments
Rear Barrel Temperature 177 - 193 °C
350 - 380 °F
Middle Barrel Temperature 177 - 193 °C
350 - 380 °F
Front Barrel Temperature 177 - 193 °C
350 - 380 °F
Mold Temperature 23.9 - 51.7 °C
75.0 - 125 °F
Back Pressure 0.345 - 1.03 MPa
50.0 - 150 psi
Descriptive Properties Value Comments
Screw Compression Ratio 2:1-3:1
Screw L/D Ratio 20:1- 24:1
Suggested Max Regrind, % 20