Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 199 - 232 °C | 390 - 450 °F | |
Multibase Multi-Pro® 0612 CW Polypropylene Calcium carbonate filler, 6% filer by weightForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Front Barrel Temperature | 199 - 232 °C | 390 - 450 °F | |
Multibase Multi-Pro® 3019 CXUW Polypropylene Calcium Carbonate Filler, 30% by weight.Features:Gloss, High Impact Resistance, GoodUV Resistance, Good Forms:PelletsProcessing Methods:Injection MoldingUses:FurnitureLawn EquipmentInformation prov.. |
|||
Front Barrel Temperature | 199 - 210 °C | 390 - 410 °F | |
RheTech Products FRG130-01 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Flame Retardant, Black Applications: Electrical component housingsSunroof componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 210 °C | 390 - 410 °F | |
RheTech Products FRP102-01 Polypropylene, Flame Retardant, Black Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 210 °C | 390 - 410 °F | |
RheTech Products FRP257-01 32% Talc Reinforced Polypropylene Copolymer, Flame Retardant, Black Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT1002-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT1055-50 Thermoplastic Polyolefin, UV Stabilized, Black Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT1055-624 Thermoplastic Polyolefin, Non-UV Stabilized, General Purpose Light Grey Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT1100-689UV Thermoplastic Polyolefin, UV Stabilized, Light Natural Beige Applications: Pillar plugsAirbag doorsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT3080-425 Thermoplastic Polyolefin, UV Stabilized, YBWA Platinum Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT3080-47UV Thermoplastic Polyolefin, UV Stabilized, AYNA Light Prairie Tan Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT3080-640UV Thermoplastic Polyolefin, UV Stabilized, BFQA Arizona Beige Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT3080-757UV Thermoplastic Polyolefin, UV Stabilized, Pueblo Gold Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products P100-01 Polypropylene Homopolymer, Black Applications: Wire harnessesTrim componentsUnderhood applicationsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products P102-00 Polypropylene, Black Applications: Consumer goodsIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products P249-01UV General Purpose Polypropylene Copolymer, UV Stabilized, Black Applications: LP bracketsSplash shieldsDoor/trunk scuffInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products P252-01 Polypropylene Copolymer, Black Applications: Cowl screenInterior trimBumper coverGlove box binInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products P254-00 Polypropylene Copolymer, Natural Applications: Air ducts - distributionInterior trimI/P componentsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products P258-01 Polypropylene Copolymer, UV Stabilized, Black Applications: Door/trunk scuffExterior grills and cowlsSteering column shroudsInterior trimInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products P261-01 Polypropylene Copolymer, Medium Impact, Black Applications: Radiator grille inlet supportElectrical housingsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products P601-01 Polypropylene Copolymer, Black Applications: Engine componentChassis componentConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products UVFT3082-74 Thermoplastic Polyolefin, 135K Flexural Modulus, UV Stabilized, Exterior DX9 Black Applications: Step padsHitch padsExterior trimInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products UVP254-01 Polypropylene Copolymer, UV Stabilized, Black Applications: Fuel filler pocketInterior trimI/P componentsCenter consoleInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 210 °C | 390 - 410 °F | |
Polymer Resources AH-GP1-[color]-H Acetal Homopolymer, Low Flow, High Melt Strength, Heat Stabilized Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Front Barrel Temperature | 199 - 210 °C | 390 - 410 °F | |
Polymer Resources AH-GP2-[color]-H Acetal Homopolymer, Medium Flow, General Purpose Molding, Heat Stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Front Barrel Temperature | 199 - 221 °C | 390 - 430 °F | |
PolyOne Dynalloy™ OBC8000-T40 Thermoplastic Elastomer (TPE) Dynalloy™ OBC8000-T40 is an easy processing, general processing TPE utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. Designed for a wide variety of applications, incl.. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products HP512-00 High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 221 °C | 390 - 430 °F | |
Ineos Nova 8048 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Improved toughness, Custom colorsApplications: Designed for injection molding applications requiring clarity and toughnessPerformance grades of polystyrene are engineered to have specific properties.. |
|||
Front Barrel Temperature | 199 - 210 °C | 390 - 410 °F | |
Polymer Resources AH-GP1 Acetal Homopolymer, Low Flow, High Melt Strength
(Unverified Data**) Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products HP501-00 High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Battery traysInterior TrimInjection molding conditions reported in table.Information provided by RheTech Products. |