Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products CC40P100-00 40% Calcium Carbonate Reinforced Polypropylene, Natural Applications: Consumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products F37-01 40% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black Applications: ElectronicsBracketsBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products F40-01 40% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black Applications: Battery traysAir cleaner housingFunctional support decksInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products F55-01 43% Glass Fiber/Talc Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Consumer goodsSupportsGolf cart bracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products G40P100-00 40% Glass Fiber Reinforced Polypropylene, Natural Injection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products G40P100-01 40% Glass Fiber Reinforced Polypropylene, Black Injection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products G40P100-04UV 40% Glass Fiber Reinforced Polypropylene, UV Stabilized, White Injection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products GC40P100-00 40% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural Applications: Consumer goodsBracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products GC40P100-01 40% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black Applications: Consumer goodsBracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products GC40P101-00 40% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural Applications: Consumer goodsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products GC43P250-00 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural Applications: Consumer goodsFunctional supportsHead lamp bracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products GC43P250-777 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Ivory Applications: BracketsStructural supportsDurable GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products GC45P200-01UV 45% Glass Fiber Reinforced Polypropylene Copolymer, UV Stabilized, Black Applications: BracketsUnderhood componentsLarge structural supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products M40P100-00 40% Mica Reinforced Polypropylene, Natural Applications: Structural componentsAir ductsFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products M40P100-01 40% Mica Reinforced Polypropylene, Black Applications: Structural componentsAir ducts and dampenersFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products M40P200-01 40% Mica Reinforced Polypropylene Copolymer, Black Applications: Automotive applicationsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products T40P100-00A 40% Talc Reinforced Polypropylene, Natural Applications: Durable goodsHVAC componentsFunctional supportsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products T40P100-01 40% Talc Reinforced Polypropylene, Black Applications: Wire troughBracketsConsolesFan shroudsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products T40P100-04 40% Talc Reinforced Polypropylene, White Applications: Automotive componentsConsumer productsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products T40P105-01 40% Talc Reinforced Polypropylene, Black Applications: Underhood componentsHVAC ductworkInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products T40P105-04 40% Talc Reinforced Polypropylene, White, 5% Titanium Dioxide Applications: Instrument cluster masksAutomotive componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products T40P106-01 40% Talc Reinforced Polypropylene, Black Applications: Underhood componentsHVAC ductworkFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products T40P108-01 40% Talc Reinforced Polypropylene, Black Applications: Wire troughBracketsConsolesFan shroudsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products T40P108-01A 40% Talc Reinforced Polypropylene, Black Applications: Underhood componentsHVAC ductworkFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products T40P109-01 40% Talc Reinforced Polypropylene, Black Applications: Underhood componentsHVAC ductworkBrackets/SupportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products T40P200-01 40% Talc Reinforced Polypropylene Copolymer, Black Applications: BracketsHousingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products T40P250-00 40% Talc Reinforced Polypropylene Copolymer, Natural Applications: BracketsHousingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
Ravago Manufacturing Americas Hylac® PL75 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products GC43P250-01 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Consumer goodsFunctional supportsHead lamp bracketsDurable GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products HP507-01 38% Talc Reinforced High Performance Polypropylene, Non-UV Stabilized, Black Applications: IP structural componentsSpeaker housingsAutomotive interior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |