Processing Properties Metric English Comments
Front Barrel Temperature 179 - 204 °C
355 - 400 °F
ExxonMobil Santoprene® 111-55 Thermoplastic Elastomer  (discontinued **)
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Front Barrel Temperature 179 - 204 °C
355 - 400 °F
ExxonMobil Santoprene® 111-64 Thermoplastic Elastomer  (discontinued **)
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Front Barrel Temperature 179 - 204 °C
355 - 400 °F
ExxonMobil Santoprene® 221-55 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide..
Front Barrel Temperature 179 - 191 °C
355 - 375 °F
Ravago Manufacturing Americas Hylac® FR134 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Front Barrel Temperature 179 - 204 °C
355 - 400 °F
Tempia Polylactic acid (PLA) Resin
A bio-degradable plastic, Polylactic acid (PLA) is made from corn. Products produced are compostable within 45 – 120 days. The degradation process of the item is temperature, humidity and thicknes..
Front Barrel Temperature 179 - 196 °C
355 - 385 °F
Elastocon TPE Technologies Elastocon® 8048N Thermoplastic Elastomer
Elastocon® 8048N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8048N is FDA compliant and well suited..
Front Barrel Temperature 179 - 196 °C
355 - 385 °F
Elastocon TPE Technologies Elastocon® 8058BL Thermoplastic Elastomer
Elastocon® 8058BL is a black lubricated thermoplastic elastomer formulated for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 8058BL is well sui..
Front Barrel Temperature 179 - 196 °C
355 - 385 °F
Elastocon TPE Technologies Elastocon® 8058HL Thermoplastic Elastomer
Elastocon® 8058HL is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 8058HL is FDA compliant a..
Front Barrel Temperature 179 - 196 °C
355 - 385 °F
Elastocon TPE Technologies Elastocon® 8058N Thermoplastic Elastomer
Elastocon® 8058N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8058N is FDA compliant and well suited..
Front Barrel Temperature 179 - 204 °C
355 - 400 °F
ExxonMobil Santoprene® 111-35 Thermoplastic Elastomer
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Front Barrel Temperature 179 - 204 °C
355 - 400 °F
ExxonMobil Santoprene® 211-45 Thermoplastic Elastomer
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
Front Barrel Temperature 179 - 196 °C
355 - 385 °F
Elastocon TPE Technologies Elastocon® 8150B Thermoplastic Elastomer
Elastocon® 8150B is a black thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8150B is well suited for consumer goods a..
Front Barrel Temperature 179 - 204 °C
355 - 400 °F
ExxonMobil Santoprene® 111-73 Thermoplastic Elastomer  (discontinued **)
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Front Barrel Temperature 179 - 204 °C
355 - 400 °F
ExxonMobil Santoprene® 111-80 Thermoplastic Elastomer  (discontinued **)
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Front Barrel Temperature 179 - 204 °C
355 - 400 °F
ExxonMobil Santoprene® 211-55 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
Front Barrel Temperature 179 - 204 °C
355 - 400 °F
ExxonMobil Santoprene® 211-64 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
Front Barrel Temperature 179 - 204 °C
355 - 400 °F
ExxonMobil Santoprene® 211-73 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
Front Barrel Temperature 179 - 204 °C
355 - 400 °F
ExxonMobil Santoprene® 211-80 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
Front Barrel Temperature 179 - 204 °C
355 - 400 °F
ExxonMobil Santoprene® 111-87 Thermoplastic Elastomer  (discontinued **)
A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Front Barrel Temperature 179 - 204 °C
355 - 400 °F
ExxonMobil Santoprene® 211-87 Thermoplastic Elastomer  (discontinued **)
A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
Front Barrel Temperature 179 - 204 °C
355 - 400 °F
ExxonMobil Santoprene® 111-45 Thermoplastic Elastomer
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..