Material Notes:
Elastocon® 8058HL is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 8058HL is FDA compliant and well suited for consumer goods and industrial applications requiring U.V. stability. Elastocon® 8058HL can be overmolded to polypropylene.Information provided by Elastocon TPE Technologies, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.03 g/cc
1.03 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.012 - 0.022 cm/cm
0.012 - 0.022 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 58
58
ASTM D2240
Tensile Strength 5.67 MPa
822 psi
ASTM D412
Elongation at Break 689 %
689 %
ASTM D412
100% Modulus 0.00198 GPa
0.287 ksi
ASTM D412
Compression Set 17 %

@Temperature 20.0 °C,
Time 79200 sec
17 %

@Temperature 68.0 °F,
Time 22.0 hour
ASTM D395B
Processing Properties Metric English Comments
Feed Temperature <= 79.4 °C
<= 175 °F
Rear Barrel Temperature 174 - 191 °C
345 - 375 °F
Front Barrel Temperature 179 - 196 °C
355 - 385 °F
Nozzle Temperature 185 - 204 °C
365 - 400 °F
Mold Temperature 21.1 - 37.8 °C
70.0 - 100 °F
Back Pressure 0.345 - 0.689 MPa
50.0 - 100 psi
Descriptive Properties Value Comments
Injection Rate Moderate to Fast
Users viewing this material also viewed the following: