Processing Properties Metric English Comments
Front Barrel Temperature 160 - 185 °C
320 - 365 °F
Huntsman AVALON® 55 AEX Thermoplastic Polyurethane
Introduction: AVALON 55 AEX is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 55 AEX is part of the AVALON Perform Range and offers a specially designed,..