Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 374 °C | 705 °F | |
Oxford Polymers PEEK 20GF-Natural PEEK, 20% Glass Fiber Reinforced Product Description: Glass Fiber (20% Reinforced), PEEK, Polyetheretherketone injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Glass fiber Special Chara.. |