Processing Properties | Metric | English | Comments |
---|---|---|---|
Cushion | 0.635 cm | 0.250 in | |
PlastiComp Complet® LCF50 - PA66 Nylon 66, 50% Long Carbon Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 50% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Cushion | 0.635 cm | 0.250 in | |
PlastiComp Complet® LCF50 - PP Homopolymer Polypropylene, 50% Long Carbon Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 50% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Cushion | 0.635 cm | 0.250 in | |
PlastiComp Complet® LGF20 - PP Homopolymer Polypropylene, 20% Long Glass Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 20% long glass fiber reinforcementInformation provided by PlastiComp, In.. |
|||
Cushion | 0.635 cm | 0.250 in | |
PlastiComp Complet® LGF30 - PP Homopolymer Polypropylene, 30% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 30% long glass fiber reinforcementInformation provided by PlastiCom.. |
|||
Cushion | 0.635 cm | 0.250 in | |
PlastiComp Complet® LGF50 - PA66 MT Nylon 66, 50% Long Glass Fiber Reinforced, Impact Modified Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 50% long glass fiber reinforcementImpact modifiedInformation provided by .. |
|||
Cushion | 0.635 cm | 0.250 in | |
PlastiComp Complet® LGF60 - PA66 Nylon 66, 60% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 60% long glass fiber reinforcementInformation provided by PlastiComp, In.. |
|||
Cushion | 0.635 cm | 0.250 in | |
PlastiComp Complet® LCF30 - PA6 Nylon 6, 30% Long Carbon Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 30% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Cushion | 0.635 cm | 0.250 in | |
PlastiComp Complet® LCF30 - PA66 Nylon 66, 30% Long Carbon Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 30% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Cushion | 0.635 cm | 0.250 in | |
PlastiComp Complet® LCF50 - TPU Rigid Thermoplastic Polyurethane, 50% Long Carbon Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 50% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Cushion | 0.635 cm | 0.250 in | |
PlastiComp Complet® LGF20 - TPU Rigid Thermoplastic Polyurethane, 20% Long Glass Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 20% long glass fiber reinforcementInformation provided by PlastiComp, Inc.. |
|||
Cushion | 0.635 cm | 0.250 in | |
PlastiComp Complet® LGF40 - TPU Rigid Thermoplastic Polyurethane, 40% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 40% long glass fiber reinforcementInformation provided by Plas.. |
|||
Cushion | 0.635 cm | 0.250 in | |
PlastiComp Complet® LGF50 - TPU Rigid Thermoplastic Polyurethane, 50% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 50% long glass fiber reinforcementInformation provided by Plas.. |
|||
Cushion | 0.635 cm | 0.250 in | |
PlastiComp Complet® LGF60 - TPU Rigid Thermoplastic Polyurethane, 60% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 60% long glass fiber reinforcementInformation provided by Plas.. |
|||
Cushion | 0.635 cm | 0.250 in | |
MRC Polymers MAXNITE™ 500 GF15 PET, 15% Glass Fiber Filled
(discontinued **) Information provided by MRC Polymers Inc. |
|||
Cushion | <= 0.635 cm | <= 0.250 in | Injection Molding |
Ineos ABS Lustran® 308 ABS, Medical Grade Lustran® ABS 308 resin is a low gloss, easy-flowing grade of ABS (acrylonitrile butadiene styrene). This injection molding grade offers a good balance of rigidity, impact strength, and abuse resi.. |
|||
Cushion | <= 0.635 cm | <= 0.250 in | Injection Molding |
Ineos ABS Lustran® 433 ABS, General-Purpose Injection Molding Grade Lustran® ABS 433 is a general-purpose injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It is a high-impact, high-gloss ABS, available only in natural (000000) and black (904000)... |
|||
Cushion | <= 0.635 cm | <= 0.250 in | Injection Molding |
Ineos ABS Lustran® 633 ABS, Injection Molding Grade Lustran® ABS 633 is a general-purpose injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It offers a good balance of physical properties, high gloss, and good moldability. Typical .. |
|||
Cushion | 0.635 cm | 0.250 in | |
MRC Polymers EMAREXâ„¢ 300 GF43 Nylon 6, 43% Glass Fiber Filled Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc. |
|||
Cushion | 0.635 cm | 0.250 in | |
MRC Polymers EMAREXâ„¢ 400 GF13 Nylon 6/6, 13% Glass Fiber Filled Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc. |
|||
Cushion | 0.635 cm | 0.250 in | |
MRC Polymers MAXTELâ„¢ 600T25 TPO, 25% Talc Filled For automotive exterior applicationsExcellent process ability and dimensional stabilityCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Polymers Inc. |
|||
Cushion | 0.635 cm | 0.250 in | |
MRC Polymers MAXTELâ„¢ 600T30IM TPO, 30% Talc Filled For automotive exterior applicationsExcellent process ability and dimensional stabilityImpact ModifiedCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Pol.. |
|||
Cushion | 0.635 cm | 0.250 in | |
MRC Polymers NAXALOYâ„¢ 793A3 GF10 PC and Polyester Blend, 10% Glass Fiber Filled 793 GF10 is available in natural and custom colors, internal and external lubricants, UV stabilizer and other modifications.Information provided by MRC Polymers Inc. |
|||
Cushion | <= 0.635 cm | <= 0.250 in | Injection Molding |
Ineos ABS Lustran® SMA 2171 SMA, Injection Molding Grade Lustran® SMA 2171 is a high heat injection molding grade of impact-modified SMA (styrene/maleic anhydride) terpolymer offering an exceptional balance of processability and performance. Lustran®.. |
|||
Cushion | 0.635 cm | 0.250 in | |
MRC Polymers EMAREXâ„¢ 400 GF33 Nylon 6/6, 33% Glass Fiber Filled Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc. |
|||
Cushion | 0.635 cm | 0.250 in | |
PlastiComp Complet® LCF50 - PA66 MT Nylon 66, 50% Long Carbon Fiber Reinforced, Impact Modified Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 50% carbon fiber reinforcementImpact modifiedInformation provided by Pla.. |
|||
Cushion | 0.635 cm | 0.250 in | |
PlastiComp Complet® LGF20 - PA66 Nylon 66, 20% Long Glass Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 20% long glass fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Cushion | 0.635 cm | 0.250 in | |
PlastiComp Complet® LGF30 - PA66 Nylon 66, 30% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 30% long glass fiber reinforcementInformation provided by PlastiComp, In.. |
|||
Cushion | 0.635 cm | 0.250 in | |
PlastiComp Complet® LGF40 - PA66 Nylon 66, 40% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 40% long glass fiber reinforcementInformation provided by PlastiComp, In.. |
|||
Cushion | 0.635 cm | 0.250 in | |
PlastiComp Complet® LGF50 - PA66 Nylon 66, 50% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 50% long glass fiber reinforcementInformation provided by PlastiComp, In.. |
|||
Cushion | 0.635 cm | 0.250 in | Average value: 0.635 cm Grade Count:3 |