Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
Multibase TPSiV® 4000-70A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; UV stableAPPLICATIONS: Solution for soft touch overmolding on consumer electronics, mob.. |
|||
Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
Multibase TPSiV® 4100-60A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Low compression setAPPLICATIONS: Solution for soft touch overmolding on consumer electr.. |
|||
Mold Temperature | 20.0 - 60.0 °C | 68.0 - 140 °F | Injection Molding |
Polimeri Europa Edistir RK 451G Polystyrene UL94 V-0, polybromobiphenylether (PBBE) free, flame retarded, high impact polystyrene. This grade combines medium flow, heat resistance and good light stability for injection moulding of technical p.. |
|||
Mold Temperature | 20.0 - 60.0 °C | 68.0 - 140 °F | Injection Molding |
Polimeri Europa Edistir SR 550 Polystyrene High impact, easy flow polystyrene with good elasticity at low temperatures.Suitable for injection moulding of large or complex parts with low thickness and high impact strength.
Designation: Thermo.. |
|||
Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
Polykemi AB POLYelast TPE Z400 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
Polykemi AB POLYelast TPE Z406 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
Polykemi AB POLYelast TPE Z900 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Mold Temperature | 20.0 - 50.0 °C | 68.0 - 122 °F | |
Polykemi AB POLYfill PPH 150DNH Polypropylene Homopolymer, Flame Retardant, Halogen Free Information provided by Polykemi AB |
|||
Mold Temperature | 20.0 - 120 °C | 68.0 - 248 °F | Injection Molding |
DuPont Performance Polymers Crastin® CE15330 BK010 PBT
(Unverified Data**) Crastin® CE15330 BK010 is a 30% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0 at 0.71mm(0.028in).Information provided by DuPont Performance.. |
|||
Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
Advanced Elastomer Systems VistaFlex® 715-N Thermoplastic Rubber
(discontinued **) Description: A black high-flow thermoplastic elastomer especially designed for injection molding applications. It replaces soft thermoplastics such as SBS, SEBS, and PVC blends. Supplied as free-f.. |
|||
Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
Termopol Termoton® K4GA4070A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |
|||
Mold Temperature | 20.0 - 50.0 °C | 68.0 - 122 °F | |
Premix Thermoplastics PRE-ELEC® PE 1270
(discontinued **) PRE-ELEC PE 1270 is a conductive thermoplastic compound based on PE-LLD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 12.. |
|||
Mold Temperature | 20.0 - 70.0 °C | 68.0 - 158 °F | Injection |
Huntsman IROGRAN® A 78 E 4723 Polyester-Based TPU-Injection Extrusion Grade Introduction: IROGRAN A 78 E 4723 is a thermoplastic polyester- polyurethane for injection moulding and extrusion applications. Additional characteristics of the product are flexibility and high mec.. |
|||
Mold Temperature | 20.0 - 70.0 °C | 68.0 - 158 °F | Injection |
Huntsman IROGRAN® A 85 P 4722 TPU-Polyester Introduction: IROGRAN A 85 P 4722 is a halogen-free thermoplastic- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are good microbial resista.. |
|||
Mold Temperature | 20.0 - 70.0 °C | 68.0 - 158 °F | Injection |
Huntsman IROGRAN® A 92 P 4637 TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | Injection Molding |
LG Chemical KEYFLEX BT 2140D Ester Type TPE Description: Injection Molding, TPC-ET, Specialty, Low ModulusApplication: Films & SheetsCAS: 37282-12-5Information provided by LG Chemical |
|||
Mold Temperature | 20.0 - 70.0 °C | 68.0 - 158 °F | Injection |
Huntsman IROGRAN® A 92 H 4656 Polyester-Based TPU-Injection Molding Grade Introduction: IROGRAN A 92 H 4656 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and e.. |
|||
Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
LATI Latistat 52/7-02 PP Homopolymer Dissipative product based on Polypropylene homopolymer (PPh). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
SK Chemicals SKYTHANE® R155D Polyether Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
SK Chemicals SKYTHANE® R180A Polyether Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Mold Temperature | 20.0 - 50.0 °C | 68.0 - 122 °F | |
Borealis BJ356MO Polypropylene Copolymer BJ356MO is a heterophasic copolymer. This grade provides very high melt flow rate, very high stiffness and medium impact strength. and is designed for high-speed injection molding and contains nucle.. |
|||
Mold Temperature | 20.0 - 70.0 °C | 68.0 - 158 °F | |
BASF Elastoblend LP 9192 TPUR Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien.. |
|||
Mold Temperature | 20.0 - 70.0 °C | 68.0 - 158 °F | |
BASF Elastollan 1085 A TPUR Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien.. |
|||
Mold Temperature | 20.0 - 70.0 °C | 68.0 - 158 °F | |
BASF Elastollan C 88 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c.. |
|||
Mold Temperature | 20.0 - 70.0 °C | 68.0 - 158 °F | |
BASF Elastollan SP 852 TPUR Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien.. |
|||
Mold Temperature | 20.0 - 50.0 °C | 68.0 - 122 °F | |
Polykemi AB POLYfill PPH DNH15025 GF10 Polypropylene Homopolymer, Flame Retardant, Halogen Free, Glass Fibre-Reinforced Information provided by Polykemi AB |
|||
Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
Wacker Silicones Geniomer® 80 Silicone TPE SLM TPSE 80 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phase.. |
|||
Mold Temperature | 20.0 - 50.0 °C | 68.0 - 122 °F | |
Eurotec® Tecolen® CP30 NL XA80 PPCP, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Mold Temperature | 20.0 - 50.0 °C | 68.0 - 122 °F | Injection-molding |
BASF Ultramid® Seal-Fit PA6/66 (Conditioned) Description: Transparent, tough, amorphous copolyamide for injection molding, specially developed for tight overmoulding of metal inlays.Information provided by BASF |