Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 15.0 - 32.0 °C | 59.0 - 89.6 °F | Injection |
Lubrizol Estane® 58123 Thermoplastic Polyurethane Features: High moisture vapor transmission with low water swell and excellent low temperature and elasticity properties.Uses: Blown and flat die/cast film extrusion, injection molding and cable jack.. |
|||
Mold Temperature | 16.0 - 32.0 °C | 60.8 - 89.6 °F | |
Eastman Eastar EN076 Copolyester Eastar Copolyester EN076 is recommended for the thick-walled containers that are prevalent in the cosmetics and personal care markets. This copolyester offers good processability with the benefits o.. |
|||
Mold Temperature | 16.0 - 32.0 °C | 60.8 - 89.6 °F | |
Eastman Eastar MN058 Copolyester Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. Eastar MN058 Copolyester is a medical gra.. |
|||
Mold Temperature | 16.0 - 32.0 °C | 60.8 - 89.6 °F | |
Eastman Eastar MN059 Copolyester Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. Eastar MN059 Copolyester is a medical gra.. |
|||
Mold Temperature | 16.0 - 32.0 °C | 60.8 - 89.6 °F | |
Eastman Eastar EN059 Copolyester, Natural Applications:Cosmetics/personal care packagingDeodorant PackagingFragrance packagingOral hygienePlastics for hygiene feminine productsToothbrushesToys/Sporting goodsWriting instrumentsProduct Descri.. |