Material Notes:
Eastar Copolyester EN076 is recommended for the thick-walled containers that are prevalent in the cosmetics and personal care markets. This copolyester offers good processability with the benefits of glass such as high clarity, brightness, and good color.Applications/UsesCosmetics/personal care packaging
Physical Properties Metric English Comments
Specific Gravity 1.32 g/cc
1.32 g/cc
ASTM D792
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 111
111
ASTM D785
Tensile Strength at Break 26.0 MPa
3770 psi
ASTM D638
Tensile Strength, Yield 56.0 MPa
8120 psi
ASTM D638
Elongation at Break 75 %
75 %
ASTM D638
Elongation at Yield 4.0 %
4.0 %
ASTM D638
Flexural Yield Strength 74.0 MPa
10700 psi
ASTM D790
Flexural Modulus 2.35 GPa
341 ksi
ASTM D790
Izod Impact, Notched 0.330 J/cm

@Temperature -40.0 °C
0.618 ft-lb/in

@Temperature -40.0 °F
ASTM D256
0.670 J/cm

@Temperature 23.0 °C
1.26 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D4812
3.20 J/cm

@Temperature -40.0 °C
5.99 ft-lb/in

@Temperature -40.0 °F
ASTM D4812
Puncture Energy 31.0 J
22.9 ft-lb
Puncture Resistance @Max Load, 23°C; ASTM D3763
45.0 J

@Temperature -40.0 °C
33.2 ft-lb

@Temperature -40.0 °F
Puncture Resistance at Max Load; ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 69.0 °C
156 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °C
144 °F
ASTM D648
Optical Properties Metric English Comments
Haze 0.80 %
0.80 %
ASTM D1003
Transmission, Visible 86 %
86 %
Regular Transmittance; ASTM D1003
89 %
89 %
Total Transmittance; ASTM D1003
Processing Properties Metric English Comments
Melt Temperature 277 - 293 °C
531 - 559 °F
Mold Temperature 16.0 - 32.0 °C
60.8 - 89.6 °F
Drying Temperature 150 °C
302 °F
Dry Time 4 - 6 hour
4 - 6 hour