Processing Properties Metric English Comments
Mold Temperature 177 - 204 °C
351 - 399 °F
Solvay Specialty Polymers AvaSpire® AV-722 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-722 is an unreinforced polyaryletherketone (PAEK) that offers improved economics relative to PEEK while retaining most of PEEK's key performance attributes. AV-722 resin has been formula..
Mold Temperature 177 - 204 °C
351 - 399 °F
Solvay Specialty Polymers AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-722 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-722. This formulation offers improved part economics relative to 30% carbon fiber reinforced PEEK while retaining most of..
Mold Temperature 177 - 204 °C
351 - 399 °F
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK)  (Unverified Data**)
Ketaspire KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provided.In..
Mold Temperature 177 - 204 °C
351 - 399 °F
Solvay Specialty Polymers KetaSpire® KT-850P Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-850P is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color coarse powder form. KetaSpire PEEK is produced to the highest industry standa..
Mold Temperature 177 - 204 °C
351 - 399 °F
Solvay Specialty Polymers KetaSpire® KT-880 GF30 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-880 GF30 is the high-flow, 30% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire..
Mold Temperature 177 - 204 °C
351 - 399 °F
Solvay Specialty Polymers AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber
AvaSpire® AV-722 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-722. This formulation offers improved part economics relative to 30% carbon fiber reinforced PEEK while retaining..
Mold Temperature 177 - 204 °C
351 - 399 °F
Solvay Specialty Polymers AvaSpire® AV-722 Polyaryletherketone (PAEK)
AvaSpire® AV-722 is an unreinforced polyaryletherketone (PAEK) that offers improved economics relative to PEEK while retaining most of PEEK's key performance attributes. AV-722 resin has been for..
Mold Temperature 177 - 204 °C
351 - 399 °F
Solvay Specialty Polymers KetaSpire® KT-820 GF15 Polyetheretherketone (PEEK), 15% Glass Fiber
KetaSpire® KT-820 GF15 is a low flow, 15% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpir..
Mold Temperature 177 - 204 °C
351 - 399 °F
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK)
KetaSpire® KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provide..
Mold Temperature 177 - 204 °C
351 - 399 °F
Solvay Specialty Polymers KetaSpire® KT-850P Polyetheretherketone (PEEK)
KetaSpire® KT-850P is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color coarse powder form. KetaSpire® PEEK is produced to the highest industr..
Mold Temperature 177 - 204 °C
351 - 399 °F
Solvay Specialty Polymers KetaSpire® KT-880 GF15 Polyetheretherketone (PEEK), 15% Glass Fiber
KetaSpire® KT-880 GF15 is a high flow, 15% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpi..
Mold Temperature 177 - 204 °C
351 - 399 °F
Solvay Specialty Polymers KetaSpire® KT-880 GF20 Polyetheretherketone (PEEK), 20% Glass Fiber
KetaSpire® KT-880 GF20 is a high flow, 20% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpi..
Mold Temperature 177 - 204 °C
351 - 399 °F
Solvay Specialty Polymers KetaSpire® KT-880 GF30 Polyetheretherketone (PEEK), 30% Glass Fiber
KetaSpire® KT-880 GF30 is the high-flow, 30% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaS..