Processing Properties Metric English Comments
Mold Temperature 188 - 199 °C
370 - 390 °F
Blow Molding
PolyOne Geon™ Vinyl Packaging 2020 LO-GC Polyvinyl Chloride, Rigid (PVC, Rigid)
Geon® 2020 LO-GC is a glass clear pellet compound designed for water bottle and other low odor appliations that require FDA sanctioned materials.Information provided by PolyOne
Mold Temperature 188 - 199 °C
370 - 390 °F
Blow Molding
PolyOne Geon™ Vinyl Packaging 2020 LO-TB Polyvinyl Chloride, Rigid (PVC, Rigid)
Geon® 2020 LO-TB is a clear blue tint pellet compound designed for water bottle and other low odor appliations that require FDA sanctioned materials.Information provided by PolyOne
Mold Temperature 177 - 199 °C
350 - 390 °F
Oxford Polymers PEEK-20CF-Black PEEK, 20% Carbon Fiber Reinforced
Product Description: Carbon Fiber (20% Reinforced), PEEK, Polyetheretherketone, injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Carbon fiber Special Ch..