Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 143 - 171 °C | 289 - 340 °F | |
PolyOne Dynaflex™ G6703-0001 Thermoplastic Elastomer (TPE) Dynaflex™ G6703-0001 is an easy processing compound designed for use in injection molding applications where extremely soft feel properties are desired. - Excellent Colorability - Good Ozone and UV.. |
|||
Rear Barrel Temperature | 143 - 160 °C | 290 - 320 °F | |
Elastocon TPE Technologies Elastocon® 8028N Thermoplastic Elastomer Elastocon® 8028N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8028N is FDA compliant and well suited.. |
|||
Rear Barrel Temperature | 143 - 160 °C | 290 - 320 °F | |
Elastocon TPE Technologies Elastocon® 8038N Thermoplastic Elastomer Elastocon® 8038N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8038N is FDA compliant and well suited.. |
|||
Rear Barrel Temperature | 143 - 160 °C | 290 - 320 °F | |
Elastocon TPE Technologies Elastocon® 8138B Thermoplastic Elastomer Elastocon® 8138B is a black thermoplastic elastomer compound formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8138B is well suited for consumer.. |