Polymer Property : Rear Barrel Temperature = 320 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Rear Barrel Temperature 149 - 160 °C
300 - 320 °F
RheTech Products E204-01 High Density Polyethylene, Black
Applications: Electrical housingsUnderhood componentsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 116 - 160 °C
241 - 320 °F
PolyOne Dynaflex™ D3204-1000-03 Thermoplastic Elastomer (TPE)
Dynaflex™ D3204-1000-03 is an easy processing TPE designed for general purpose applications and is suitable for injection molding, extrusion, blow molding, and thermoforming processes. - Dry Feel -..
Rear Barrel Temperature 140 - 160 °C
284 - 320 °F
Injection Molding
Stellarchem MP-835B TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Rear Barrel Temperature 150 - 160 °C
302 - 320 °F
Extrusion
Stellarchem SV-B40D TPV Compound
This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on ..
Rear Barrel Temperature 150 - 160 °C
302 - 320 °F
Extrusion
Stellarchem SV-B65E TPV Compound
This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on ..
Rear Barrel Temperature 150 - 160 °C
302 - 320 °F
Extrusion
Stellarchem SV-B70E TPV Compound
This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on ..
Rear Barrel Temperature 150 - 160 °C
302 - 320 °F
Extrusion
Stellarchem SV-B75E TPV Compound
This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on ..
Rear Barrel Temperature 150 - 160 °C
302 - 320 °F
Extrusion
Stellarchem SV-B80E TPV Compound
This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on ..
Rear Barrel Temperature 150 - 160 °C
302 - 320 °F
Extrusion
Stellarchem SV-B87E TPV Compound
This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on ..
Rear Barrel Temperature 138 - 160 °C
280 - 320 °F
Elastocon TPE Technologies Elastocon® 2810 Thermoplastic Elastomer
Elastocon® 2810 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® 2810 is FDA compliant and well suit..
Rear Barrel Temperature 138 - 160 °C
280 - 320 °F
Elastocon TPE Technologies Elastocon® 2825 Thermoplastic Elastomer
Elastocon® 2825 thermoplastic elastomer compound has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® 2825 is FDA compliant and ..
Rear Barrel Temperature 143 - 160 °C
290 - 320 °F
Elastocon TPE Technologies Elastocon® 8028N Thermoplastic Elastomer
Elastocon® 8028N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8028N is FDA compliant and well suited..
Rear Barrel Temperature 143 - 160 °C
290 - 320 °F
Elastocon TPE Technologies Elastocon® 8038N Thermoplastic Elastomer
Elastocon® 8038N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8038N is FDA compliant and well suited..
Rear Barrel Temperature 143 - 160 °C
290 - 320 °F
Elastocon TPE Technologies Elastocon® 8138B Thermoplastic Elastomer
Elastocon® 8138B is a black thermoplastic elastomer compound formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8138B is well suited for consumer..
Rear Barrel Temperature 149 - 160 °C
300 - 320 °F
RheTech Products E204-00 High Density Polyethylene, Natural
Applications: Electrical housingsUnderhood componentsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products.