Processing Properties Metric English Comments
Rear Barrel Temperature 254 - 274 °C
490 - 525 °F
PTS Tristar® PC-10R-(14) 14 MFI Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 254 - 274 °C
490 - 525 °F
PTS Tristar® PC-10R-(VE) 12 MFI UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 254 - 274 °C
490 - 525 °F
PTS Tristar® PC-10FR 12 MFI Flame Retardant Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 254 - 274 °C
490 - 525 °F
PTS Tristar® PC-10FR-(V) 12 MFI Flame Retardant, UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 254 - 274 °C
490 - 525 °F
PTS Tristar® PC-10FR-(VIM) 12 MFI Flame Retardant, UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 254 - 274 °C
490 - 525 °F
PTS Tristar® PC-10FRN (V) 15 MFI, 5VA, Flame Retardant, UV Stabilized Polycarbonate With Release
ROHS Compliant.Information provided by Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 254 - 274 °C
490 - 525 °F
PTS Tristar® PC-10FRN 15 MFI Flame Retardant Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 254 - 274 °C
490 - 525 °F
PTS Tristar® PC-10FRNH 12 MFI Non-Bromine Non-Chlorine Flame Retardant Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 254 - 274 °C
490 - 525 °F
PTS Tristar® PC-10FRNH-V 12 MFI Non-Bromine Non-Chlorine Flame Retardant UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 232 - 274 °C
450 - 525 °F
Star Plastics PC/ABSQX7002 Molding Grade PC/ABS High Flow
Information provided by Star Plastics, Inc.
Rear Barrel Temperature 238 - 274 °C
460 - 525 °F
Star Plastics PC/ABSQX7005 Molding Grade PC/ABS
Information provided by Star Plastics, Inc.
Rear Barrel Temperature 246 - 274 °C
475 - 525 °F
Star Plastics PC20NBR Molding Grade PC with Release
Information provided by Star Plastics, Inc.
Rear Barrel Temperature 246 - 274 °C
475 - 525 °F
Star Plastics PC721HFR Molding Grade PC
Information provided by Star Plastics, Inc.
Rear Barrel Temperature 246 - 274 °C
475 - 525 °F
Star Plastics PC721HFR Molding Grade PC High Flow with Release
Information provided by Star Plastics, Inc.
Rear Barrel Temperature 246 - 274 °C
475 - 525 °F
Star Plastics PC7523R Molding Grade PC
Information provided by Star Plastics, Inc.
Rear Barrel Temperature 254 - 274 °C
490 - 525 °F
Samyang Trirex® PC-3025U 12 MFI UV Stabilized Clear Polycarbonate
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 246 - 274 °C
475 - 525 °F
CTC X-PRO PP 100 P1015 Polypropylene Homopolymer
X-PRO PP 1015 is a polypropylene homopolymer. Its applications are: general purpose industrial injection molding, virgin polypropylene diluents, and polymer base for glass, talc or specialty filled..