Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TP-FR IM2 PBT, Impact Modified, Flame Retardant, High Flow Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Rear Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TP-FRG7.5 Polybutylene Terephthalate, 7 1/2 % Glass Reinforced, Flame Retardant Polybutylene Terephthalate, 7 1/2 % Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Rear Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TP-FRHG15 Polybutylene Terephthalate, 15% Glass Reinforced Alloy, Flame Retardant Polybutylene Terephthalate, 15% Glass Reinforced Alloy, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
Rear Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TP-FRHG30 Polybutylene Terephthalate, 30% Glass Reinforced Alloy, Flame Retardant Polybutylene Terephthalate, 30% Glass Reinforced Alloy, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
Rear Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TP-FR-IM Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low Flow Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa.. |
|||
Rear Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TP-FR-IM2-[color]-6 Polybutylene Terephthalate, Low Temperature Impact Modified, Flame Retardant Polybutylene Terephthalate, Low Temperature Impact Modified, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, t.. |
|||
Rear Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TP-G10 Polybutylene Terephthalate, 10% Glass Reinforced Polybutylene Terephthalate, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
Rear Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TP-G30-TFE15 Polybutylene Terephthalate, 30% Glass Reinforced, 15% PTFE Polybutylene Terephthalate, 30% Glass Reinforced, 15% PTFEProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Rear Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TP-HG15 Polybutylene Terephthalate, 15% Glass Reinforced Alloy Polybutylene Terephthalate, 15% Glass Reinforced AlloyProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informatio.. |
|||
Rear Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TP-IG30 Polybutylene Terephthalate, 30% Glass Reinforced, Reduced Warpage Polybutylene Terephthalate, 30% Glass Reinforced, Reduced WarpageProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Rear Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TP-IGFR-G30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant, Reduced Warpage Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant, Reduced WarpageProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmen.. |
|||
Rear Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TP-IM-G15 Polybutylene Terephthalate, 15% Glass Reinforced, Impact Modified Polybutylene Terephthalate, 15% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Rear Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TP-IM-G30 Polybutylene Terephthalate, 30% Glass Reinforced, Impact Modified Polybutylene Terephthalate, 30% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Rear Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TP-IM-G7.5 Polybutylene Terephthalate, 7.5% Glass Reinforced, Impact Modified Polybutylene Terephthalate, 7.5% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample.. |
|||
Rear Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TPSF-FR1 PBT, 30% Glass Reinforced Structural Foam Grade, Flame Retardant Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel.. |
|||
Rear Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TPSF-FRG10 Polybutylene Terephthalate, Structural Foam, 10% Glass Reinforced, Flame Retardant Polybutylene Terephthalate, Structural Foam, 10% Glass Reinforced, Flame RetardantProcess: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, .. |
|||
Rear Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TPSF-FRG30 Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced, Flame Retardant Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced, Flame RetardantProcess: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, .. |
|||
Rear Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TPSF-G30 Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf.. |
|||
Rear Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TPSF-GP1 PBT, 30% Glass Reinforced Structural Foam Grade Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel.. |
|||
Rear Barrel Temperature | 238 - 254 °C | 460 - 489 °F | |
LNP VALOX® SMV5846 PBT + PET Alloy, 20% Carbon Fiber Reinforcement
(discontinued **) ESD ApplicationsFeatures: Good Chemical Resistance, High Flow, Flame RetardantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is .. |
|||
Rear Barrel Temperature | 238 - 266 °C | 460 - 510 °F | |
Ravago Manufacturing Americas Hybrid B2026IU Polycarbonate + PBT Alloy Available in North America UV Stabilizer Good Impact Resistance RoHS Compliant Form: Pellets Processing Method: Injection Molding Information provided by Ravago |
|||
Rear Barrel Temperature | 238 - 249 °C | 460 - 480 °F | |
Firestone C200-001 Nylon 6 Natural color. Not heat stabilized, modified, or lubricated. Chip size is 2 x 3.5 mm.Information provided by Firestone |
|||
Rear Barrel Temperature | 238 - 249 °C | 460 - 480 °F | |
Firestone C212-15C Nylon 6, Heat Stabilized Off white color. Heat stabilized, Modified, and Lubricated. Chip size is 2 x 3.5 mm.Information provided by Firestone |
|||
Rear Barrel Temperature | 238 - 249 °C | 460 - 480 °F | |
Firestone CLM200-001 Nylon 6 Used for monofiliament extrusion. Natural color. Not heat stabilized or modified. Lubricated. Chip size is 2 x 3.5 mm.Information provided by Firestone |
|||
Rear Barrel Temperature | 238 - 249 °C | 460 - 480 °F | |
Firestone CR212-203-D Nylon 6, Heat Stabilized Black color. Heat stabilized, Modified, and Lubricated. Chip size is 2 x 3 mm.Information provided by Firestone |
|||
Rear Barrel Temperature | 238 °C | 460 °F | |
Styron MAGNUMâ„¢ 375 HH Acrylonitrile Butadiene Styrene (ABS) Resin Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection moldingApplications: Automotive interior trim applications requiring low volatile organic compounds (VOC)Information provided by.. |
|||
Rear Barrel Temperature | 238 °C | 460 °F | |
Styron MAGNUMâ„¢ 375 HP Acrylonitrile Butadiene Styrene (ABS) Resin Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection molded automotive interior trim applications.Applications: Chrysler-MSDB-191Ford-WSB-M4D690-AGM-GMP.ABS.009Information provided .. |
|||
Rear Barrel Temperature | 238 - 282 °C | 460 - 540 °F | |
Wellman Wellamid® 42LH XE-N Unfilled Nylon 6, Lubricated & Heat Stabilized Typical Applications: Automotive seat belt, buckle and anchor components; convoluted tubing for wire harnesses; furniture hardware, curtain glides.Data provided by the manufacturer, Wellman Inc. |
|||
Rear Barrel Temperature | 238 - 257 °C | 460 - 495 °F | |
Diamond Polymers ASA/PC FA-30 Description: ASA Weatherable Polymer, Injection Molding Grade, Flame RetardantInformation provided by Diamond Polymers, Inc. |
|||
Rear Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Engineered Polymer Solutions PBT VM 450, 20% Mineral Filled Plate-able. Natural and colors available. Injection molding grade. Uses: Automotive, appliancesInformation provided by Engineered Polymer Solutions. |