Polymer Property : Rear Barrel Temperature = 421 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Rear Barrel Temperature 360 - 421 °C
680 - 790 °F
LNP ULTEM® EXCP0096 Polyetherimide, 30% Carbon Fiber Reinforcement, 10% PTFE Lubricant  (discontinued **)
Features: Lubricated, Electrically Conductive, Good Wear Resistance, High Heat ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This dat..
Rear Barrel Temperature 360 - 421 °C
680 - 790 °F
LNP ULTEM® UC3000 Polyetherimide, 30% Carbon Fiber Reinforcement  (discontinued **)
High modulus with shielding/ conductive characteristics for high-heat applications.Features: Electrically Conductive, High Heat Resistance, High StrengthForms: PelletsProcessing Method: Injection Mo..
Rear Barrel Temperature 360 - 421 °C
680 - 790 °F
LNP ULTEM® UCF1205 Polyetherimide, 12% Carbon Fiber Reinforcement, 5% PTFE Lubricant  (discontinued **)
Office equipment internal parts.Features: Lubricated, Good Wear ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labe..
Rear Barrel Temperature 360 - 421 °C
680 - 790 °F
LNP ULTEM® SMU5831 Polyetherimide, 30% CarbonGlassMineral Reinforced  (discontinued **)
ESD characteristics for ultra high-heat applications. Will be UC3010H.Features: High Heat ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Compa..
Rear Barrel Temperature 360 - 421 °C
680 - 790 °F
LNP ULTEM® SMU5832 Polyetherimide, 30% CarbonGlassMineral Reinforced  (discontinued **)
ESD characteristics for ultra high-heat applications. Will be UC3010.Features: High Heat ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Compan..
Rear Barrel Temperature 360 - 421 °C
680 - 790 °F
LNP ULTEM® SMU5852 Polyetherimide, 30% Carbon Fiber Reinforcement, 15% PTFE Lubricant  (discontinued **)
Features: Lubricated, Electrically Conductive, Good Wear ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Dis..
Rear Barrel Temperature 360 - 421 °C
680 - 790 °F
LNP ULTEM® SMU5834 Polyetherimide, 20% Carbon Fiber Reinforcement  (discontinued **)
High modulus with shielding/ conductive characteristics for high-heat applications.Features: Electrically Conductive, High Heat Resistance, High StrengthForms: PelletsProcessing Method: Injection Mo..
Rear Barrel Temperature 360 - 421 °C
680 - 790 °F
LNP ULTEM® SMU5835 Polyetherimide, 25% Carbon Fiber Reinforcement  (discontinued **)
High modulus with shielding/ conductive characteristics for high-heat applications.Features: Electrically Conductive, High Heat Resistance, High StrengthForms: PelletsProcessing Method: Injection Mo..
Rear Barrel Temperature 360 - 421 °C
680 - 790 °F
LNP ULTEM® SMU5836 Polyetherimide, 30% Carbon Fiber Reinforcement  (discontinued **)
High modulus with shielding/ conductive characteristics for high-heat applications.Features: Electrically Conductive, High Heat Resistance, High StrengthForms: PelletsProcessing Method: Injection Mo..