Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 221 - 254 °C | 430 - 490 °F | |
Polymer Resources PC/ABS-FR1 Flame Retardant PC/ABS Alloy PC/ABS Alloy, Flame Retardant, Standard FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided.. |
|||
Rear Barrel Temperature | 221 - 254 °C | 430 - 490 °F | |
Polymer Resources PC/ABS-FR2 Flame Retardant PC/ABS Alloy, High Flow PC/ABS Alloy, Flame Retardant, Higher FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided b.. |
|||
Rear Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TP-FR IM PBT, Impact Modified, Flame Retardant, Low Flow Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Rear Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TP-FR IM2 PBT, Impact Modified, Flame Retardant, High Flow Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Rear Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TP-FRG30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant Polybutylene Terephthalate, 30% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Rear Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TP-FRHG15 Polybutylene Terephthalate, 15% Glass Reinforced Alloy, Flame Retardant Polybutylene Terephthalate, 15% Glass Reinforced Alloy, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
Rear Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TP-FRHG30 Polybutylene Terephthalate, 30% Glass Reinforced Alloy, Flame Retardant Polybutylene Terephthalate, 30% Glass Reinforced Alloy, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
Rear Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TP-FR-IM Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low Flow Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa.. |
|||
Rear Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TP-FR-IM-[color]-3 Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low Flow Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa.. |
|||
Rear Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TP-FR-IM2 Polybutylene Terephthalate, Impact Modified, Flame Retardant, High Flow Polybutylene Terephthalate, Impact Modified, Flame Retardant, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
Rear Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TP-FR-IM2-[color]-6 Polybutylene Terephthalate, Low Temperature Impact Modified, Flame Retardant Polybutylene Terephthalate, Low Temperature Impact Modified, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, t.. |
|||
Rear Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TP-FV699 PBT, 10% Glass Reinforced Structural Foam Grade, Low Shrinkage Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel.. |
|||
Rear Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TP-G20 Polybutylene Terephthalate, 20% Glass Reinforced Polybutylene Terephthalate, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
Rear Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TP-G40 Polybutylene Terephthalate, 40% Glass Reinforced Polybutylene Terephthalate, 40% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
Rear Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TP-HG15 Polybutylene Terephthalate, 15% Glass Reinforced Alloy Polybutylene Terephthalate, 15% Glass Reinforced AlloyProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informatio.. |
|||
Rear Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TP-HG30 Polybutylene Terephthalate, 30% Glass Reinforced Alloy Polybutylene Terephthalate, 30% Glass Reinforced AlloyProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informatio.. |
|||
Rear Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TP-IG30 Polybutylene Terephthalate, 30% Glass Reinforced, Reduced Warpage Polybutylene Terephthalate, 30% Glass Reinforced, Reduced WarpageProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Rear Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TP-IM-G30 Polybutylene Terephthalate, 30% Glass Reinforced, Impact Modified Polybutylene Terephthalate, 30% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Rear Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TPSF-FRG30 Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced, Flame Retardant Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced, Flame RetardantProcess: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, .. |
|||
Rear Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TPSF-G10 Polybutylene Terephthalate, Structural Foam, 10% Glass Reinforced Polybutylene Terephthalate, Structural Foam, 10% Glass ReinforcedProcess: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Info.. |
|||
Rear Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TPSF-GP1 PBT, 30% Glass Reinforced Structural Foam Grade Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel.. |
|||
Rear Barrel Temperature | 238 - 254 °C | 460 - 489 °F | |
LNP VALOX® SMV5845 PBT + PET Alloy, 16% Carbon Fiber Reinforcement
(discontinued **) ESD Applications. Will be VC1600.Features: Good Chemical Resistance, High Flow, Flame RetardantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.Th.. |
|||
Rear Barrel Temperature | 238 - 254 °C | 460 - 489 °F | |
LNP VALOX® SMV5846 PBT + PET Alloy, 20% Carbon Fiber Reinforcement
(discontinued **) ESD ApplicationsFeatures: Good Chemical Resistance, High Flow, Flame RetardantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is .. |
|||
Rear Barrel Temperature | 221 - 254 °C | 430 - 490 °F | |
Polymer Resources PC/ABS-FR1-[color]-UV Flame Retardant PC/ABS Alloy, UV-stabilized PC/ABS Alloy, Flame Retardant, Standard Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Rear Barrel Temperature | 241 - 254 °C | 465 - 490 °F | |
Teknor Apex Beetle® 102 Nylon 66, Unreinforced, Nucleated Notes: Nucleated for fast cycling; Improved strength and rigidity; FMVSS Flammability: Passes, FMVSS 302Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex |
|||
Rear Barrel Temperature | 241 - 254 °C | 465 - 490 °F | |
Teknor Apex Chemlon® 100 L Nylon 66, Unreinforced Notes: Internally and externally lubricated; General Purpose; Double-lubricated for improved part ejection and machine feed Processing Method: Injection Molding Forms: PelletsInformation Provided by.. |
|||
Rear Barrel Temperature | 241 - 254 °C | 465 - 490 °F | |
Teknor Apex Chemlon® 100 W Nylon 66, Unreinforced Notes: MoS2 modified; Molybdenum disulphide modified to provide self-lubrication and low friction to parts subjected to wear and abrasion. FMVSS Flammability: Passes, FMVSS 302Processing Method: Inj.. |
|||
Rear Barrel Temperature | 241 - 254 °C | 465 - 490 °F | |
Teknor Apex Chemlon® 104 Nylon 66, Impact Grade Notes: Medium-Impact; General Purpose; Impact modified to provide excellent toughness Processing Method: Injection Molding Forms: Pellets Automotive Specifications: Chrysler MS-DB41 CPN3992 Color: W.. |
|||
Rear Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Engineered Polymer Solutions PBT VM 450, 20% Mineral Filled Plate-able. Natural and colors available. Injection molding grade. Uses: Automotive, appliancesInformation provided by Engineered Polymer Solutions. |
|||
Rear Barrel Temperature | 249 - 254 °C | 480 - 490 °F | |
Diamond Polymers ASA M-143 Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc. |