Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 232 - 266 °C | 450 - 511 °F | Injection Molding |
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (DAM) Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce.. |
|||
Rear Barrel Temperature | 232 - 266 °C | 450 - 511 °F | Injection Molding |
Ineos ABS Triax® 1185 ABS/Nylon Alloy, Injection Molding Grade Triax® 1185 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with excellent processability, good chemical resistance, g.. |
|||
Rear Barrel Temperature | 232 - 266 °C | 450 - 511 °F | Injection Molding |
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (Conditioned) Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce.. |