Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
Polymer Resources PC/TP-FR2 Flame Retardant PC/Polyester Alloy Flame Retardant, High Impact, Excellent Chemical ResistanceFeatures: • Flame Retardant • Impact Modified • Self Extinguishing • Good Chemical ResistanceProcess: Injection MoldingNotes: All p.. |
|||
Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
Polymer Resources PC/TP-GP1-[color]-3 PC Polyester, High Impact, Good Chemical Resistance, UV-stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
Polymer Resources PC/TP-GP1-HF PC/Polyester Alloy, High Melt Flow High Melt Flow, Good Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by .. |
|||
Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
Polymer Resources PC/TP-GP2 PC/Polyester Alloy High Impact, Excellent Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided b.. |
|||
Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
Polymer Resources PC/TP-GP3-G10 PC/Polyester Alloy, 10% Glass Reinforced Superior Chemical Resistance, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
Polymer Resources PC-FD4-[color]-1 Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig.. |
|||
Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
Polymer Resources PC-GP4-[color]-3 Polycarbonate, UV-stabilized, Easy Flow Polycarbonate, UV-stabilized, Easy FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P.. |
|||
Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
Polymer Resources PC-GP4-[color]-5 Polycarbonate, FDA-compliant Feedstocks, Easy Flow Polycarbonate, FDA-compliant Feedstocks, Easy FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Rear Barrel Temperature | 221 - 271 °C | 430 - 520 °F | |
Polymer Resources PPX-MF-FR1 Modified-PPO, V-0 Flame Retardant, Mineral Reinforced Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDT, Mineral ReinforcedFeatures: • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mecha.. |
|||
Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
Polymer Resources PC/TP-GP2 PC Polyester, High Impact, Excellent Chemical Resistance
(Unverified Data**)& Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
Oxford Polymers PC C20-000 Clear PC Product Description: Amorphous, Unreinforced Polycarbonate injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Pigment onlySpecial Characteristics: Easy fl.. |
|||
Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
Polymer Resources PC-UV4 Polycarbonate, UV-stabilized, Easy Flow Polycarbonate, UV-stabilized, Easy FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P.. |
|||
Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
Polymer Resources PC-UV4-[color]-1 Polycarbonate, UV-stabilized, Easy Flow with Mold Release Polycarbonate, UV-stabilized, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
PTS Tristar® PC-10FR-(16) 16 MFI Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
PTS Tristar® PC-10FR-(V16) 16 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
PTS Tristar® PC-15R-113 15 MFI Clear Utility Grade Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
LTL Color Compounds ColorFast® PC200 Polycarbonate 20 melt superior processing, fast cyclingAll information provided by LTL Color Compounders, Inc. |
|||
Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
Mitsubishi Iupilon® S3000R 16.5 MFI Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
Mitsubishi Iupilon® S3000UR 16.5 MFI, UV Stabilized Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
Mitsubishi Iupilon® S3001R 16.5 MFI FDA Compliant Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
MRC Polymers EMAREXâ„¢ 300 GF33 Nylon 6, 33% Glass Fiber Filled Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc. |
|||
Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
MRC Polymers EMAREXâ„¢ 300 GF43 Nylon 6, 43% Glass Fiber Filled Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc. |
|||
Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
MRC Polymers NAXALOYâ„¢ 770 ABS + PC Alloy Impact modifiedAvailable in Natural, Black, and GrayCan be Colored (Masterbatch)Low temperature ductility and impact modifiedCan be UV StabilizedInternal and external lubricant can be addedInformati.. |
|||
Rear Barrel Temperature | 260 - 271 °C | 500 - 520 °F | |
MRC Polymers NAXALOYâ„¢ 770 GF10 ABS+PC Alloy, 10% Glass Fiber Filled Can be UV StabilizedInternal and external lubricant can be addedInformation provided by MRC Polymers Inc. |
|||
Rear Barrel Temperature | 260 - 271 °C | 500 - 520 °F | |
MRC Polymers NAXALOYâ„¢ 770 GF16 ABS+PC Alloy, 16% Glass Fiber Filled Can be UV StabilizedInternal and external lubricant can be addedInformation provided by MRC Polymers Inc. |
|||
Rear Barrel Temperature | 260 - 271 °C | 500 - 520 °F | |
MRC Polymers NAXELLâ„¢ PC210MR General Purpose Polycarbonate, Medium MFR, with Release Medium melt without impact modificationMFR can be modified between 10 to 40 g/10minCan be UV stabilizedInternal and external lubricant can be addedGenerally for black and gray colors onlyFR package .. |
|||
Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
MRC Polymers NAXELLâ„¢ PC23M-10G General Purpose Polycarbonate, 10% Glass Fiber Filled, Low Viscosity Can be impact modifiedInternal and external lubricant can be addedBlack onlyInformation provided by MRC Polymers Inc. |
|||
Rear Barrel Temperature | 243 - 271 °C | 470 - 520 °F | |
Star Plastics PC/PBTQX7008 Molding Grade PC/PBT Information provided by Star Plastics, Inc. |
|||
Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
Samyang Trirex® PC-3022IR 15 MFI Clear Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
Samyang Trirex® PC-3022U 15 MFI UV Stabilized Clear Polycarbonate Information provided by US distributor Polymer Technology and Services, LLC (PTS). |