Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 60.0 - 62.8 °C | 140 - 145 °F | |
LTL Color Compounds Surlyn Reflection Series® SURSG201UG Surlyn Resin/Nylon 6 Alloy A patented alloy of DuPont™ Surlyn® resin and nylon 6 for applications that require a high gloss, molded in color surface finish directly from the mold.All information provided by LTL Color .. |