Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 60.0 - 80.0 °C @Time 7200 - 14400 sec |
140 - 176 °F @Time 2.00 - 4.00 hour |
Pre-drying |
Premix Thermoplastics PRE-ELEC® PP 1385 PRE-ELEC PP 1385 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Drying Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Pre-drying |
Premix Thermoplastics PRE-ELEC® PS 1331 Carbon Black Filled Conductive Thermoplastic Compound PRE-ELEC® PS 1331 is a carbon black filled conductive thermoplastic compound based on polystyrene. In addition to a low electrical resistivity PRE-ELEC® PS 1331 has excellent mechanical properties.. |
|||
Drying Temperature | 60.0 °C | 140 °F | |
Pasargad Polymer Peyvand Pasadur 3P-H8130B PBT, 30% Glass Fiber Reinforced Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Automotive Exterior PartsAutomotive Interior PartsInformation provided by Pasargad Poly.. |
|||
Drying Temperature | 60.0 - 70.0 °C | 140 - 158 °F | |
LG Chemical HI855H PMMA, Impact Resistant Grade Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che.. |
|||
Drying Temperature | 60.0 - 70.0 °C | 140 - 158 °F | |
LG Chemical IF850 PMMA, General Purpose Grade for Injection Molding High flowability gradeParticularly recommended for complicated profiles or large and thin wall partsFeatures: Excellent transparency and eleganceWeather resistance and chemical resistanceSurface har.. |
|||
Drying Temperature | 60.0 - 62.8 °C | 140 - 145 °F | |
LTL Color Compounds Surlyn Reflection Series® SURSG201UG Surlyn Resin/Nylon 6 Alloy A patented alloy of DuPont™ Surlyn® resin and nylon 6 for applications that require a high gloss, molded in color surface finish directly from the mold.All information provided by LTL Color .. |
|||
Drying Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Pre drying temp. |
Supreme Petrochem SP 554 Flame Retardant Polystyrene Characteristics Very good flow properties Good balance of toughness and rigidity Processing Molding Gas assist molding Applications Large size T.V. Cabinets VCR cabinets Electrical boxes, electr.. |
|||
Drying Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Pre drying temp. |
Supreme Petrochem SP 564 Flame Retardant Polystyrene Characteristics Very good flow properties Free of DBDPO, PBDE & TBBA, complies with ROHS directive of EU Processing MoldingApplications Large size T.V. Cabinets VCR cabinets Electrical boxes, ele.. |
|||
Drying Temperature | 60.0 - 70.0 °C | 140 - 158 °F | |
Arkema Group Pebax® 4033 SP 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 4033 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide.. |