Polymer Property : Drying Temperature = 180 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Drying Temperature 180 - 204 °C
356 - 400 °F
Average value: 196 °C Grade Count:5
Overview of materials for Thermoplastic Polyimide, Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyimide, Carbon Fiber". Each property range of values reported is minimum and maximum va..
Drying Temperature 180 °C
356 °F
Lubrizol Estane® ZHF 90AT0 Thermoplastic Polyurethane, Flame Retardant
Type: Estane® ZHF 90AT0 TPU is a clear, glossy, zero halogen flame retardant polyether based thermoplastic polyurethane compound.Features: Outstanding TPU properties.Uses: Cable jacket and tube/hos..
Drying Temperature 180 °C
356 °F
ExxonMobil Santoprene® 8221-75M300 Thermoplastic Elastomer
A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for automotive interior applications requiring low fogging and ..