Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 116 - 140 °C | 240 - 284 °F | Average value: 124 °C Grade Count:17 |
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35.. |
|||
Drying Temperature | 120 - 140 °C @Time 14400 - 21600 sec |
248 - 284 °F @Time 4.00 - 6.00 hour |
Pre-dry |
Kingfa PBT-RG302 Flame Retardant, 30% Glass Fiber Reinforced PBT Features:Flame retardantHigh strengthHigh temperature propertiesHigh glossyGood surfaceNo bloomingApplications:Injection moldingConnectorsRelayBobbinsPlugsE & E partsInformation Provided by Kingfa S.. |
|||
Drying Temperature | 120 - 140 °C | 248 - 284 °F | |
Eurotec® Tecopet® PT70 GR15 NL100 PR PET, 15% glass fiber reinforced, heat stabilized, natural, fast crystallization grade Information provided by Eurotec® |
|||
Drying Temperature | 120 - 140 °C | 248 - 284 °F | |
Eurotec® Tecopet® PT70 GR30 NL100 PR PET, 30% glass fiber reinforced, high heat stabilized, natural, fast crystallization grade Information provided by Eurotec® |
|||
Drying Temperature | 120 - 140 °C | 248 - 284 °F | |
Eurotec® Tecopet® PT74 CR20 BK111 PR PET, 20% carbon fiber reinforced, black, fast crystallization grade Information provided by Eurotec® |
|||
Drying Temperature | 120 - 140 °C | 248 - 284 °F | |
Asia International Enterprise (Hong Kong) 30G3 Polybutylene terephthalate, 15% Glass Fiber Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Drying Temperature | 130 - 140 °C | 266 - 284 °F | Temperature can be reduced when using vacuum ovens. |
LATI LARTON CE/60 60% Special Mineral Filled Polyphenylene sulfide (PPS)
(Unverified Data**) Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex.. |