Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 166 - 177 °C @Time 14400 sec |
331 - 351 °F @Time 4.00 hour |
|
Solvay Specialty Polymers Radel® R-7535 Polyphenylsulfone (PPSU) Radel® R-7535 polyphenylsulfone resin is a cost-effective solution for aircraft interior applications. This product complies with the FAA regulation 14CFR Part 25 Appendix F, offering vertical bu.. |
|||
Drying Temperature | 166 - 177 °C @Time 14400 sec |
331 - 351 °F @Time 4.00 hour |
|
Solvay Specialty Polymers Radel® R-7558 Polyphenylsulfone (PPSU) Radel® R-7558 polyphenylsulfone resin is a cost-effective solution for aircraft interior applications. This product complies with the FAA regulation 14CFR Part 25 Appendix F, offering vertical bu.. |
|||
Drying Temperature | 166 - 177 °C @Time 14400 sec |
331 - 351 °F @Time 4.00 hour |
|
Solvay Specialty Polymers Radel® R-7625 Polyphenylsulfone (PPSU) Radel® R-7625 polyphenylsulfone resin is a cost-effective solution for aircraft interior applications that offers improved UV resistance versus Radel® R-7535 and Radel® R-7558. The product .. |