Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | |
PolyOne Stat-Tech™ PC-CB2/000 CR Polycarbonate (PC) Stat-Tech™ PC-CB2/000 CR XP100827Information provided by PolyOne |
|||
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | |
PolyOne Versollan™ RU 2205-1 Thermoplastic Elastomer (TPE) Versollan™ RU 2205-1 is the first of a new class of high performance, injection moldable TPU alloys developed to offer a rubbery feel and appearance, reduced cycle times, combined with the performa.. |
|||
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | |
Polymer Resources NY66-G43 Nylon 66, 43% Glass Reinforced Nylon 66, 43% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test.. |
|||
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | |
Polymer Resources NY66-G43-[color]-H Nylon 66, 43% Glass Reinforced, Heat Stabilized Nylon 66, 43% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylo.. |
|||
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | |
Polymer Resources NY66-GP1 General Purpose Nylon 66 General Purpose Nylon 66, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry.. |
|||
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | |
Polymer Resources NY66-IM2-G33 Nylon 66, 33% Glass Reinforced, Impact Modified Nylon 66, 33% Glass Reinforced, Impact Modified, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylo.. |
|||
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | |
Polymer Resources NY6-G43 Nylon 6, 43% Glass Reinforced Nylon 6, 43% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste.. |
|||
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | |
Polymer Resources PC-HM-FR2-[color]-1 Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold Release Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa.. |
|||
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | |
Polymer Resources PPX-GP3-[color]-EN Modified-PPO, Extrusion Grade Modified-Polyphenylene Oxide, Extrusion Grade, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: ExtrusionNotes: All physical, mechanical and thermal testing conduct.. |
|||
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | |
Polymer Resources TP-G30-TFE15 Polybutylene Terephthalate, 30% Glass Reinforced, 15% PTFE Polybutylene Terephthalate, 30% Glass Reinforced, 15% PTFEProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | Extrusion Molding |
LG Chemical KEYFLEX BT 3038D Ester Type TPE Description: Injection Molding, TPC-ET, Functional, Fast Molding, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |
|||
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | Extrusion Molding |
LG Chemical KEYFLEX BT 3055D Ester Type TPE Description: Injection Molding, TPC-ET, Functional, Fast Molding, Medium ModulusApplication: Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Dry Time | 3.00 - 6.00 hour | 3.00 - 6.00 hour | Injection Molding |
LG Chemical LUCEL N127LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
Dry Time | 3.00 - 5.00 hour | 3.00 - 5.00 hour | Injection Molding |
LG Chemical LUCON PN9009 PPS+MF Injection Molding Grade, PPS+MF, High Thermal Conductivity, Chemical Resistance, High Heat ResistanceApplication: Electrical or Electronic Parts (Heat sink, LED etc.) Motor HousingCAS No. 25212-74-2.. |
|||
Dry Time | 3.00 - 5.00 hour | 3.00 - 5.00 hour | Injection Molding |
LG Chemical LUPOY GP1006FM PC, Flame Retardant Description: Injection Molding, PC, Flame RetardantApplication: IT/OA, E&E Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical |
|||
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | |
Styron EMERGEâ„¢ 7100 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS) Overview: EMERGEâ„¢ PC/ABS 7100 advanced resin exhibits a balance of properties between impact strength, heat resistance and processability. Its superior natural base color and lot-to-lot color .. |
|||
Dry Time | 3.00 hour | 3.00 hour | Injection |
Alliance Polymers Viprene™ G90A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G90A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | |
Arkema Group Pebax® Clear 400 Polyether Block Amide (PEBA) Pebax® Clear 400 combines high transparency level with the unique performance of Pebax®, thermoplastic elastomer made of flexible polyether and rigid polyamide.Information provided by Arkema Group.. |
|||
Dry Time | 3.00 - 5.00 hour | 3.00 - 5.00 hour | Injection Molding |
LG Chemical LUPOY SC1004ML PC, High Impact Description: Injection Molding, PC, General Purpose, High Impact, Good Coloring, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 9046-16-6Information provided by LG Chemical.. |