Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Resources PC-HM-FR2-[color]-1 Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold Release

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 10% Glass Filled , Polycarbonate, Glass Fiber Filled, Flame Retardant
Manufacturer Polymer Resources, LTD
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polymer Resources PC-HM-FR2-[color]-1 Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold Release.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
ASTM D955
Melt Flow 8.0 - 16 g/10 min

@Load 1.20 kg,
Temperature 300 °C
8.0 - 16 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 65.5 MPa
9500 psi
ASTM D638
Tensile Strength, Yield 55.8 MPa
8100 psi
ASTM D638
Flexural Strength 103 MPa
14900 psi
ASTM D790
Flexural Modulus 3.38 GPa
490 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm

@Temperature 22.8 °C
2.00 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 143 °C
290 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 138 °C
280 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
Processing Properties Metric English Comments
Rear Barrel Temperature 293 - 316 °C
560 - 600 °F
Middle Barrel Temperature 304 - 327 °C
580 - 620 °F
Front Barrel Temperature 316 - 338 °C
600 - 640 °F
Melt Temperature 302 - 329 °C
575 - 625 °F
Mold Temperature 82.2 - 116 °C
180 - 240 °F
Drying Temperature 118 - 124 °C
245 - 255 °F
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Descriptive Properties Value Comments
Vent 0.0005